MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ASI® MP 55300 Methacrylate adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: MP55300 is a high performance two part methacrylate adhesive engineered to bond a wide range of plastics, metals, and composite assemblies. It offers outstanding bond strength, is extremely durable, with excellent impact and weathering properties. MP55300 increases the reliability of finished assemblies with exceptional flexibility, its ability to withstand extreme temperature fluctuation and thermal cycling, and resistance to a wide range of chemicals and environmental conditions. It offers exceptional bonding to a wide range of substrates.

Substrates bonded include ABS, Acrylic, Aluminum, Nylon, Phenolic, Polycarbonate, Polystyrene, PVC, Steel, Stainless metals, coated metals, fiberglass, phenolics, gel coats, epoxy, rim urethane, polyurethane, liquid molding resins, PPO's, Vinyl, PEEK, PBT Blends, and PET Blends.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.983 g/cc0.0355 lb/in³uncured, mixed
Viscosity  60000 cP
@Temperature 25.0 °C
60000 cP
@Temperature 77.0 °F
resin, uncured
 60000 cP
@Temperature 25.0 °C
60000 cP
@Temperature 77.0 °F
activator, uncured
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 17.2 MPa>= 2500 psicured
Shear Strength >= 17.2 MPa>= 2500 psicured
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flash Point 10.6 °C51.0 °Funcured
 
Processing PropertiesMetricEnglishComments
Working Life 4.00 min4.00 min
 
Descriptive Properties
Color / appearanceoff white, amber sheen. Uncured
Gap Fillup to 0.125 inches. Cured
Handling Strength10 minutes, cured
Mix Ratio1 to 1. (Vol or wt). Uncured
Thix Index5. Uncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1060 Steel, as rolled
AISI 1022 Steel, normalized at 925°C (1700°F)
AISI 1021 Steel, cold rolled, 25 mm (1 in.) round
Ensinger Tecapeek® XP98 XRO Polyetheretherketone (PEEK), compression molded, 30% carbon fiber filled, x-ray opaque
Ascend Performance Materials Vydyne® R533H BK0667 Nylon 66/610 Copolymer, 33% Glass Filled

PASINC9016 / 233383

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.