AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent creep resistance and low moisture absorption are also characteristic of this resin. AMODEL A-1115 HS resin can be easily processed using conventional equipment and methods.This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001. MatWeb has an entry for this material conditioned at 50% RH. |