MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mapal Plastics Maplon Type K OPAQLON COO1 Polypropylene Sheet
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Sheet/Thermoforming Grade

Material Notes: Maplon Catalog No. L050-C001K0101 is an extremely opaque white sheet. Sheet surface is smoothly embossed with similar finish on both sides..

Main advantages: High opacity, High rigidity high thermal and chemical resistance, Good weather resistance, No yellowing after exposure to light, Good print-ability in all printing methods: offset UV and conventional, screen UV and solvent based
Main disadvantages: Due to sheet hardness it requires high pressure in die cutting, Material is not recommended for box production

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.960 g/cc0.960 g/cc
Thickness 500 microns19.7 mil
Surface Tension >= 48 dynes/cm>= 48 dynes/cmCorona treated on both sides, After 2 months from production in original packaging
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7272ISO/R 868
Film Tensile Strength at Yield, MD 37.0 MPa
@Temperature 23.0 °C
5370 psi
@Temperature 73.4 °F
ASTM D638
Film Tensile Strength at Yield, TD 36.0 MPa
@Temperature 23.0 °C
5220 psi
@Temperature 73.4 °F
ASTM D638
Film Elongation at Break, MD 50 %
@Temperature 23.0 °C
50 %
@Temperature 73.4 °F
ASTM D638
Film Elongation at Break, TD 16 %
@Temperature 23.0 °C
16 %
@Temperature 73.4 °F
ASTM D638
Film Elongation at Yield, MD 15 %
@Temperature 23.0 °C
15 %
@Temperature 73.4 °F
ASTM D638
Film Elongation at Yield, TD 12 %
@Temperature 23.0 °C
12 %
@Temperature 73.4 °F
ASTM D638
Modulus of Elasticity 0.570 GPa
@Temperature 23.0 °C
82.7 ksi
@Temperature 73.4 °F
MD/TD; ASTM D638
Tear Strength <= 230 kN/m<= 1310 pliMapal internal
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 155 °C311 °FASTM D1525
Heat Distortion Temperature 110 °C230 °FASTM 648
 
Optical PropertiesMetricEnglishComments
Transmission, Visible >= 99.5 %>= 99.5 %Measured in daylight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mapal Plastics Maplon Type 3G Polypropylene Sheet
Mapal Plastics Maplon CFA-HK Polypropylene Sheet
Mapal Plastics Maplon PAPER MATCH Polypropylene Sheet
Mapal Plastics Maplon Type D Polypropylene Sheet
Mapal Plastics Maplon Type H Polypropylene Sheet

PMAPAL06 / 83617

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.