MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Red Brass, UNS C23000 (230 Brass), OSO50 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Good to excellent corrosion resistance. Excellent cold workability; good hot formability.

Applications: weather-stripping, conduit, sockets, fasteners, fire extinguishers, condenser and heat exchanger tubing, plumbing pipe, radiator cores.

Test specimen: flat products - 1mm thickness.

Key Words: CDA 230, CZ102, ISO CuZn15, CEN CW502L, gilding metal, 85/15 brass
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.75 g/cc0.316 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell F 5959
Hardness, Rockwell 30T 1414
Tensile Strength, Ultimate 275 MPa39900 psi
Tensile Strength, Yield 83.0 MPa12000 psi
Elongation at Break 47 %47 %In 50 mm
Modulus of Elasticity 115 GPa16700 ksi
Poissons Ratio 0.3070.307
Machinability 30 %30 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 44.0 GPa6380 ksi
Shear Strength 215 MPa31200 psi
Izod Impact 43.0 J31.7 ft-lbCast and annealed
 45.0 J33.2 ft-lbCast
Charpy Impact 69.0 J50.9 ft-lbKeyhole, annealed rod, specific temper not reported
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.00000470 ohm-cm
@Temperature 20.0 °C
0.00000470 ohm-cm
@Temperature 68.0 °F
 0.0000299 ohm-cm
@Temperature 1100 °C
0.0000299 ohm-cm
@Temperature 2010 °F
liquid phase
Magnetic Susceptibility -1.00e-6-1.00e-6Approximately, cgs units
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.7 µm/m-°C
@Temperature 20.0 - 300 °C
10.4 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 159 W/m-K
@Temperature 20.0 °C
1100 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 990 - 1025 °C1810 - 1877 °F
Solidus 990 °C1810 °F
Liquidus 1025 °C1877 °F
Annealing Point 427 - 732 °C800 - 1350 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 425 - 725 °C797 - 1340 °F
Hot-Working Temperature 800 - 900 °C1470 - 1650 °F
Recrystallization Temperature 350 °C
@Thickness 1.00 mm
662 °F
@Thickness 0.0394 in
Approximately
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 84 - 86 %84 - 86 %
Iron, Fe >= 0.050 %>= 0.050 %
Lead, Pb >= 0.060 %>= 0.060 %
Zinc, Zn 15 %15 %
 
Descriptive Properties
Velocity of Sound3660 m/sat 20°C

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Red Brass, UNS C23000 (230 Brass), OSO70 Temper flat products
Red Brass, UNS C23000 (230 Brass), OSO35 Temper flat products
Red Brass, UNS C23000 (230 Brass), OSO25 Temper flat products
Red Brass, UNS C23000 (230 Brass), OSO15 Temper flat products
Red Brass, UNS C23000 (230 Brass), H01 Temper flat products

MC23000b3 / 11034

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.