MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Guarniflon MFA Fluoropolymer
Categories: Polymer; Thermoplastic; Fluoropolymer; TFE/Perfluoromethylvinylether Copolymer (MFA)

Material Notes: It’s a semi-crystalline fully-fluorinated melt processable fluoropolymer which offer the highest temperature rating and broadest chemical resistance of all melt processable fluoropolymers. It is an ideal choice for extreme thermal and chemical environments. MFA exhibits the outstanding thermal behaviour and chemical resistance found in PTFE, PFA and FEP. In addition, parts made with MFA have been shown to have smooth finished surfaces. This makes MFA a good candidate for the semiconductor, electronics and biologic applications.

Information provided by Guarniflon®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.12 - 2.17 g/cc0.0766 - 0.0784 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 55 - 6055 - 60ASTM D2240
Tensile Strength >= 25.0 MPa>= 3630 psiASTM D638
Elongation at Break >= 300 %>= 300 %ASTM D638
Flexural Modulus 0.600 GPa87.0 ksiASTM D790
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 30.0 - 40.0 kV/mm762 - 1020 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 120 - 200 µm/m-°C
@Temperature 25.0 - 100 °C
66.7 - 111 µin/in-°F
@Temperature 77.0 - 212 °F
ASTM D696
Thermal Conductivity 0.240 W/m-K1.67 BTU-in/hr-ft²-°FASTM D177
Melting Point 260 - 290 °C500 - 554 °F
Maximum Service Temperature, Air 250 °C482 °F
Minimum Service Temperature, Air -200 °C-328 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1100 (Heated 593°C)
Iron Thermocouple Wire Type J - Standard
Constantan Thermocouple Wire
AGC Fluon® ETFE
Hexcel® HexMC® C/2000/R1A Carbon Epoxy Molding Composite

PGUARN021 / 142754

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.