MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Colour Image Plastic Compound Electroblend® ABS-2801 ABS, Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Carbon Fiber Reinforced

Material Notes: Product Description: Electroblend® ABS-2801 is a carbon fiber reinforced, flame retardant polycarbonate compound. This grade offers good Moldability and electrically conductive.

Features:

  • Carbon Fiber
  • Electrically conductive
  • Good moldability
Uses:
  • Automotive industry
  • Electrical/Electronic components parts
  • Business machines
Forms:
  • Pellets
Processing Method:
  • Injection Molding

Information provided by Colour Image Plastic Compound Sdn Bhd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/ccASTM D792
Water Absorption 0.15 %
@Time 86400 sec
0.15 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.00040 - 0.0010 cm/cm
@Thickness 3.20 mm
0.00040 - 0.0010 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 134 MPa19400 psiASTM D638
Elongation at Break 2.3 %2.3 %ASTM D638
Tensile Modulus 9.483 GPa1375 ksiASTM D638
Flexural Strength 193 MPa28000 psiASTM D790
Flexural Modulus 7.79 GPa1130 ksiASTM D790
Izod Impact, Notched 1.19 J/cm2.23 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1000 ohm - 1e+051000 ohm - 1e+05ASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 133 °C
@Thickness 4.00 mm
271 °F
@Thickness 0.157 in
Unannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 240 - 250 °C464 - 482 °F
Front Barrel Temperature 250 - 260 °C482 - 500 °F
Nozzle Temperature 260 - 270 °C500 - 518 °F
Melt Temperature 250 - 270 °C482 - 518 °F
Mold Temperature 80.0 - 120 °C176 - 248 °F
Drying Temperature 90.0 - 100 °C194 - 212 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOLO081 / 265973

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.