MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Phillips 66 SynXPA® 32 Turbine Oil
Categories: Fluid; Lubricant; Synthetic Ether Base

Material Notes: Description: Conoco SynXPATurbine Oil meets the severe-service requirements of industrially rated stationary and marine-turbine power plants. It is formulated with premium-quality synthetic-ester base oils that offer exceptional detergency and affinity for metal surfaces, excellent low-temperature fluidity and superior high-temperature thermal stability. These oils are blended with select ashless additives to produce excellent load-carrying capacity, superior high-temperature corrosion protection and oxidation stability. When changing from another product to SynXPA Turbine Oil, flushing the system is recommended to remove contaminants and moisture. Mixing conventional and SynXPA Turbine Oil is not recommended.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 111111Viscosity Index
Saybolt Viscosity at 100°F 127.3 SUS127.3 SUS
Saybolt Viscosity at 210°F 42.6 SUS42.6 SUS
Kinematic Viscosity at 40°C (104°F) 26.8 cSt26.8 cSt
Kinematic Viscosity at 100°C (212°F) 4.98 cSt4.98 cSt
 
Thermal PropertiesMetricEnglishComments
Pour Point -56.1 °C-69.0 °F
Flash Point 260 °C500 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON191 / 75228

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.