MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Solvay FM® 6604-1 BMI Foaming Adhesive
Categories: Polymer; Adhesive; Thermoset; Bismaleimide (BMI)

Material Notes: Description: FM® 6604-1 is a modified bismaleimide (BMI) resin core splice foaming adhesive. It has a cure temperature of 350°F (177°C) with a post-cure at 440°C (227°C). The service temperature is -67°F to 450°F (-57°C to 232°C) with post-cure.

Features & Benefits:

  • Maximum continuous service temperature up to 450°F (232°C) with post-cure
  • Expansion ratio 2:1 nominal
  • Ideal for non-metallic core splice and edge closeout
  • Long-term aging
  • Fuel tight
  • High strength-to-density ratio
  • Structural equivalency to unspliced core
Applications:
  • Core shear-ties
  • Edge closeouts
  • Insert bonding

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.480 g/cc0.0173 lb/in³
Volatiles <= 2.0 %<= 2.0 %
Storage Temperature -18.0 °C-0.400 °F
 
Mechanical PropertiesMetricEnglishComments
Shear Strength  1.79 MPa
@Temperature 232 °C
260 psi
@Temperature 450 °F
Beam
 2.21 MPa
@Temperature 204 °C
320 psi
@Temperature 399 °F
Beam
 3.65 MPa
@Temperature 232 °C
530 psi
@Temperature 450 °F
Tube
 3.79 MPa
@Temperature 24.0 °C
550 psi
@Temperature 75.2 °F
Beam
 4.34 MPa
@Temperature -55.0 °C
630 psi
@Temperature -67.0 °F
Beam
 4.41 MPa
@Temperature 204 °C
640 psi
@Temperature 399 °F
Tube
 6.21 MPa
@Temperature 24.0 °C
900 psi
@Temperature 75.2 °F
Tube
 6.55 MPa
@Temperature -55.0 °C
950 psi
@Temperature -67.0 °F
Tube
 6.89 MPa
@Temperature 24.0 °C
1000 psi
@Temperature 75.2 °F
Tube, 1,1,1 trichloroethane soak per MIL-T-81533 vapor
 8.96 MPa
@Temperature 24.0 °C
1300 psi
@Temperature 75.2 °F
Tube, 30-day salt spray per ASTM B-117 at 95°F (35°C)
 9.65 MPa
@Temperature 24.0 °C
1400 psi
@Temperature 75.2 °F
Tube, 72-hour water boil in demineralized water
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 232 °C450 °F
Minimum Service Temperature, Air -57.0 °C-70.6 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorBrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Henkel Hysol EA 9833.1 (BMI) Core Splice Adhesive
Evonik Compimide® TM123 4,4'-Bis(o-propenylphenoxy)benzophenone
Solvay HTM® 556 BMI
Henkel Hysol EA 9673 (BMI) Film Adhesive
Evonik Compimide® 353A Bismaleimide

PCYTED045 / 180347

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.