Celanese FORTRON 1115L0 PPS, 15% Specialty
Categories:
Polymer
;
Thermoplastic
;
Polyphenylene Sulfide (PPS)
;
Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
Material Notes:
Fortron« 1115L0 is a 15% fiberglass-reinforced grade of polyphenylene sulfide with high melt strength suitable for blow molding and extrusion applications.
Information provided by Celanese
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.44
g/cc
0.0520
lb/in³
ISO 1183
Water Absorption at Saturation
0.020 %
0.020 %
ISO 62
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
120
MPa
17400
psi
5mm/min; ISO 527-2/1A
Elongation at Break
2.0 %
2.0 %
5mm/min; ISO 527-2/1A
Tensile Modulus
7.70
GPa
1120
ksi
50mm/min; ISO 527-2/1A
Flexural Strength
200
MPa
29000
psi
ISO 178
Flexural Modulus
7.50
GPa
1090
ksi
ISO 178
Izod Impact, Notched (ISO)
5.20
kJ/m²
2.47
ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched
3.20
J/cm²
15.2
ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched
0.500
J/cm²
2.38
ft-lb/in²
ISO 179/1eA
Electrical Properties
Metric
English
Comments
Surface Resistance
>=
1.00e+15
ohm
>=
1.00e+15
ohm
IEC 60093
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
220
°C
428
°F
ISO 75-1, -2
Deflection Temperature at 8.0 MPa
115
°C
239
°F
ISO 75-1, -2
Processing Properties
Metric
English
Comments
Processing Temperature
140
-
160
°C
284
-
320
°F
cavity
330
-
340
°C
626
-
644
°F
hot runner
Feed Temperature
60.0
-
80.0
°C
140
-
176
°F
Zone 1
290
-
300
°C
554
-
572
°F
Zone 2
310
-
320
°C
590
-
608
°F
Zone 3
330
-
340
°C
626
-
644
°F
Zone 4
330
-
340
°C
626
-
644
°F
Die Temperature
310
-
330
°C
590
-
626
°F
Melt Temperature
330
-
340
°C
626
-
644
°F
Drying Temperature
80.0
-
100
°C
176
-
212
°F
Dry Time
3.00
-
4.00
hour
3.00
-
4.00
hour
Moisture Content
<= 0.020 %
<= 0.020 %
Injection Pressure
50.0
-
100
MPa
7250
-
14500
psi
Hold Pressure
30.0
-
70.0
MPa
4350
-
10200
psi
Back Pressure
<=
3.00
MPa
<=
435
psi
Screw Speed
50
rpm
@Diameter 55.0 mm
50
rpm
@Diameter 2.17 in
75
rpm
@Diameter 40.0 mm
75
rpm
@Diameter 1.57 in
120
rpm
@Diameter 25.0 mm
120
rpm
@Diameter 0.984 in
Descriptive Properties
Injection speed
fast
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Celanese FORTRON 205 PPS, Unfilled
Celanese FORTRON 1115E7 PPS, Glass Reinforced
Celanese FORTRON 1140L4 PPS, 40% Glass Reinforced
Celanese FORTRON 1130L4 PPS, 30% Glass Reinforced
Celanese FORTRON 1120L4 PPS, 20% Specialty
PHCQ264 / 178719
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.