MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

American Port Orford Cedar Wood
Categories: Wood and Natural Products; Wood; Softwood

Material Notes: Sometimes known as Port Oxford Cedar. Softwood. Easy to work with hand tools. Data is based on small, clear, air-dried samples unless specified.

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Chamaecyparis lawsoniana; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.400 g/cc0.0145 lb/in³Oven Dry Weight/Unseasoned Volume
 0.577 g/cc0.0208 lb/in³Unseasoned*
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 2100 N472 lb (f)Side. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 2500 N562 lb (f)End. Force required to imbed a 0.444 inch steel ball to one-half its diameter
Tensile Strength, Ultimate 1.65 MPa240 psiPerpendicular to Grain*
Modulus of Rupture 0.0469 GPa6.80 ksiStatic Bending*
 0.0780 GPa11.3 ksiIn Bending
Flexural Yield Strength 26.9 MPa3900 psiFiber Stress at Elastic Limit; Static Bending*
 53.1 MPa7700 psiBending stress at proportional limit
Flexural Modulus 9.00 GPa1310 ksiIn Bending
 10.3 GPa1500 ksiStatic Bending*
Compressive Strength 2.62 MPa380 psiPerpendicular to Grain*
 20.5 MPa2970 psiParallel to Grain*
 22.6 MPa3280 psiMax Crushing Strength Parallel to Grain*
 44.8 MPa6500 psiParallel to Grain
Shear Strength 6.07 MPa880 psiParallel to Grain*
Impact 2.72.7in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 93009300psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.00407 J/cm³0.590 in-lb/in³Static Bending*
Work to Maximum Load 0.0538 J/cm³7.80 in-lb/in³Static Bending*
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.102 W/m-K0.710 BTU-in/hr-ft²-°FOven Dry
 0.122 W/m-K0.850 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 4.6 %4.6 %Radial; Unseasoned to Oven Dry*
 6.9 %6.9 %Tangential; Unseasoned to Oven Dry*
 10.6 %10.6 %Volumetric; Unseasoned to Oven Dry*

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Eastern Red Cedar Wood
American Alaska Cedar (Yellow Cedar) Wood
American Cedar Wood
American Pine Wood
American Red Spruce Wood

PTSAA / 71284

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.