MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

HGC-2-C Precious dental alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy

Key Words: medical, surgical
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 17.3 g/cc0.625 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 105105soft
 125125hardened
Tensile Strength, Ultimate 400 MPa58000 psisoft
Tensile Strength, Yield 410 MPa59500 psihardened
 230 MPa
@Strain 0.2 %
33400 psi
@Strain 0.2 %
soft
 240 MPa
@Strain 0.2 %
34800 psi
@Strain 0.2 %
hardened
Elongation at Break 18 %18 %hardened
 20 %20 %soft
 
Thermal PropertiesMetricEnglishComments
CTE, linear 13.6 µm/m-°C
@Temperature 25.0 - 600 °C
7.56 µin/in-°F
@Temperature 77.0 - 1110 °F
Melting Point 1285 - 1370 °C2345 - 2500 °F
Solidus 1285 °C2345 °F
Liquidus 1370 °C2500 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 0.00 - 5.0 %0.00 - 5.0 %
Gold, Au 50 - 73 %50 - 73 %
Indium, In <= 2.0 %<= 2.0 %
Iridium, Ir <= 0.10 %<= 0.10 %
Palladium, Pd <= 1.0 %<= 1.0 %
Platinum, Pt <= 1.9 %<= 1.9 %
Rhenium, Re <= 0.10 %<= 0.10 %
Silver, Ag 10 - 28 %10 - 28 %
Zinc, Zn 12 - 14 %12 - 14 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
HGC-1 Precious dental alloy
LGC-4-C Precious dental alloy
HGC-4 Precious dental alloy
Gold, Au; 18K, White Composition Spec (UNS P00275)
Gold, Au; 18K, Yellow (UNS P00255)

MMEDIC35 / 12411

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.