MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Celanese Celstran® PA66-SF50-02 AF3001 Nylon 66, 50% Stainless Steel Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Stainless Steel Filled; EMI Grade

Material Notes: The Celstran PA66-SF50-02 AF3001 Natural is a 50% by weight stainless steel fiber concentrate. This product is intended to be used at levels from 6% to 40% in combination with neat or filled PA66 to achieve the desired level of electrostatic dissipation (ESD) and electromagnetic interference (EMI)/ radio frequency interference (RFI) shielding. The resulting formulation will yield stainless steel levels of 3% to 20%.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.99 g/cc0.0719 lb/in³ISO 1183
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °F10°C/min; ISO 11357-1,-2,-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature <= 320 °C<= 608 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Stat-Tech™ NN-30GF-15SS Nylon 6/6 - 30% Glass Fiber - 15% Stainless Steel
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade
RTP Company RTP 299 X 146804 A Nylon 6/6 (PA); Glass Bubbles - Preliminary Datasheet
Celanese Celstran® PA66-SF10-02 PA66, 10% Stainless Steel Reinforced
Boron, B

PHCQ180 / 178635

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.