MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Laramid K/40 HM PPA, 40% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), Carbon Fiber Filled

Material Notes: Semi-aromatic polyamide (PPA) based compound. Carbon fiber. High tensile modulus. Very good thermal properties. Good chemical resistance. Low moisture absorption.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³
Linear Mold Shrinkage, Flow 0.00050 - 0.0020 cm/cm0.00050 - 0.0020 in/in
Linear Mold Shrinkage, Transverse 0.0030 - 0.0055 cm/cm0.0030 - 0.0055 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  140 MPa
@Temperature 150 °C
20300 psi
@Temperature 302 °F
 190 MPa
@Temperature 120 °C
27600 psi
@Temperature 248 °F
 245 MPa
@Temperature 90.0 °C
35500 psi
@Temperature 194 °F
 265 MPa
@Temperature 60.0 °C
38400 psi
@Temperature 140 °F
 290 MPa
@Temperature 23.0 °C
42100 psi
@Temperature 73.4 °F
Elongation at Break  0.80 %
@Temperature 23.0 °C
0.80 %
@Temperature 73.4 °F
 1.0 %
@Temperature 60.0 °C
1.0 %
@Temperature 140 °F
 1.3 %
@Temperature 90.0 °C
1.3 %
@Temperature 194 °F
 2.0 %
@Temperature 120 °C
2.0 %
@Temperature 248 °F
 3.5 %
@Temperature 150 °C
3.5 %
@Temperature 302 °F
Tensile Modulus  12.0 GPa
@Temperature 150 °C
1740 ksi
@Temperature 302 °F
 20.0 GPa
@Temperature 120 °C
2900 ksi
@Temperature 248 °F
 27.0 GPa
@Temperature 90.0 °C
3920 ksi
@Temperature 194 °F
 32.0 GPa
@Temperature 60.0 °C
4640 ksi
@Temperature 140 °F
 36.0 GPa
@Temperature 23.0 °C
5220 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched 6.00 J/cm²28.6 ft-lb/in²
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 100 ohm-cm100 ohm-cm
Surface Resistance 10 ohm10 ohm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Deflection Temperature at 0.46 MPa (66 psi) 290 °C554 °F
Deflection Temperature at 1.8 MPa (264 psi) 280 °C536 °F
Vicat Softening Point 275 °C
@Load 5.00 kg
527 °F
@Load 11.0 lb
 
Processing PropertiesMetricEnglishComments
Melt Temperature 310 - 340 °C590 - 644 °F
Mold Temperature 150 - 170 °C302 - 338 °F
Drying Temperature 120 - 130 °C
@Time 10800 sec
248 - 266 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultraform® N2520 XL2 Electrically Conductive POM
LATI Latigloss 57 G/60 F2 PPA, 60% Glass Fiber Reinforced
LATI Latigray 82-03 CW/95 PA 12, Metallic Reinforced
Overview of materials for 6000 Series Aluminum Alloy
Overview of materials for Polyphthalamide (PPA), Carbon Fiber

PLATH9627 / 177323

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.