MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Taro Plast Tarolox 111 G6 Y0 PET, 30% Glass Fiber Reinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant

Material Notes: PET medium viscosity, 30% glass fibers reinforced, halogen free flame retardant UL94 V0, heat stabilized, designed according to RoHS Decree. Available: all colors, UV stabilized (L).

Information provided by Taro Plast S.p.a.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.59 g/cc0.0574 lb/in³ISO 1183
Filler Content 30 %30 %ISO 3451
Water Absorption 0.050 %
@Time 86400 sec
0.050 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/inISO 2577
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 105 MPa15200 psiISO 527
Elongation at Break 1.6 %1.6 %ISO 527
Tensile Modulus 12.3 GPa1780 ksiISO 527
Flexural Strength 150 MPa21800 psiISO 178
Flexural Modulus 11.0 GPa1600 ksiISO 178
Izod Impact, Notched  0.700 J/cm
@Temperature -20.0 °C
1.31 ft-lb/in
@Temperature -4.00 °F
127x12.7x3.2; ASTM D256
 0.850 J/cm
@Temperature 23.0 °C
1.59 ft-lb/in
@Temperature 73.4 °F
127x12.7x3.2; ASTM D256
Charpy Impact Unnotched 4.20 J/cm²20.0 ft-lb/in²80x10x4; ISO 179/1eU
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²80x10x4; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 600 V600 VMethod A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 µm/m-°C11.1 µin/in-°FISO 11359
Maximum Service Temperature, Air 150 °C
@Time 72000 sec
302 °F
@Time 20.0 hour
IEC 60216
Hot Ball Pressure Test 245 °C473 °FIEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 235 °C455 °FISO 75/A
Vicat Softening Point 237 °C
@Load 5.00 kg
459 °F
@Load 11.0 lb
ISO 306
Flammability, UL94 V-0
@Thickness 0.750 mm
V-0
@Thickness 0.0295 in
127x2.17xThickness
Glow Wire Ignition Temperature 775 °C
@Thickness 1.00 mm
1430 °F
@Thickness 0.0394 in
60x60xThickness; IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
60x60xThickness; IEC 60695-2-12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTARO095 / 283203

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.