MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 66, Unreinforced, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.02 - 1.67 g/cc0.0368 - 0.0603 lb/in³Average value: 1.20 g/cc Grade Count:146
 1.03 - 1.03 g/cc
@Temperature 280 - 280 °C
0.0372 - 0.0372 lb/in³
@Temperature 536 - 536 °F
Average value: 1.03 g/cc Grade Count:1
Water Absorption 0.0500 - 9.00 %0.0500 - 9.00 %Average value: 2.35 % Grade Count:95
Moisture Absorption at Equilibrium 0.170 - 3.10 %0.170 - 3.10 %Average value: 2.10 % Grade Count:44
Water Absorption at Saturation 7.00 - 9.00 %7.00 - 9.00 %Average value: 7.97 % Grade Count:13
Viscosity Number 150 - 205 cm³/g1.50 - 2.05 dl/gAverage value: 174 cm³/g Grade Count:5
Linear Mold Shrinkage 0.00100 - 0.0280 cm/cm0.00100 - 0.0280 in/inAverage value: 0.0136 cm/cm Grade Count:133
Linear Mold Shrinkage, Transverse 0.00100 - 0.0200 cm/cm0.00100 - 0.0200 in/inAverage value: 0.0128 cm/cm Grade Count:36
Melt Flow 4.00 - 130 g/10 min4.00 - 130 g/10 minAverage value: 49.8 g/10 min Grade Count:7
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 55.0 - 93.055.0 - 93.0Average value: 78.7 Grade Count:12
Hardness, Rockwell R 90.0 - 12590.0 - 125Average value: 116 Grade Count:43
Ball Indentation Hardness 55.0 - 150 MPa7980 - 21800 psiAverage value: 120 MPa Grade Count:11
Tensile Strength, Ultimate 30.0 - 137 MPa4350 - 19900 psiAverage value: 70.2 MPa Grade Count:91
 24.0 - 116 MPa
@Temperature -40.0 - 80.0 °C
3480 - 16800 psi
@Temperature -40.0 - 176 °F
Average value: 49.0 MPa Grade Count:7
 10.0 - 95.0 MPa
@Temperature -20.0 - 100 °C
1450 - 13800 psi
@Temperature -4.00 - 212 °F
Average value: 49.0 MPa Grade Count:1
 10.0 - 95.0 MPa
@Strain 1.00 - 3.00 %
1450 - 13800 psi
@Strain 1.00 - 3.00 %
Average value: 49.0 MPa Grade Count:1
Tensile Strength, Yield 32.0 - 193 MPa4640 - 28000 psiAverage value: 69.6 MPa Grade Count:77
Elongation at Break 2.20 - 300 %2.20 - 300 %Average value: 30.7 % Grade Count:126
 45.0 - 80.0 %
@Temperature 60.0 - 150 °C
45.0 - 80.0 %
@Temperature 140 - 302 °F
Average value: 89.7 % Grade Count:4
Elongation at Yield 2.00 - 25.0 %2.00 - 25.0 %Average value: 11.2 % Grade Count:49
Modulus of Elasticity 0.703 - 12.4 GPa102 - 1800 ksiAverage value: 2.89 GPa Grade Count:79
 0.400 - 3.50 GPa
@Temperature 40.0 - 150 °C
58.0 - 508 ksi
@Temperature 104 - 302 °F
Average value: 1.37 GPa Grade Count:5
Flexural Yield Strength 29.0 - 276 MPa4210 - 40000 psiAverage value: 96.5 MPa Grade Count:111
 38.0 - 170 MPa
@Temperature -40.0 - 80.0 °C
5510 - 24700 psi
@Temperature -40.0 - 176 °F
Average value: 92.9 MPa Grade Count:3
Flexural Modulus 0.255 - 12.4 GPa37.0 - 1800 ksiAverage value: 2.81 GPa Grade Count:117
 0.400 - 4.30 GPa
@Temperature -40.0 - 80.0 °C
58.0 - 624 ksi
@Temperature -40.0 - 176 °F
Average value: 2.03 GPa Grade Count:3
Compressive Yield Strength 35.0 - 98.0 MPa5080 - 14200 psiAverage value: 80.3 MPa Grade Count:4
Poissons Ratio 0.360 - 0.4000.360 - 0.400Average value: 0.387 Grade Count:9
Shear Strength 56.0 - 66.0 MPa8120 - 9570 psiAverage value: 61.8 MPa Grade Count:5
Izod Impact, Notched 0.290 - 7.47 J/cm0.543 - 14.0 ft-lb/inAverage value: 0.916 J/cm Grade Count:78
 0.350 - 1.38814 J/cm
@Temperature -40.0 - -40.0 °C
0.656 - 2.60056 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 0.728 J/cm Grade Count:4
 0.427 - 0.427 J/cm
@Temperature -40.0 - -40.0 °C
0.800 - 0.800 ft-lb/in
@Temperature -40.0 - -40.0 °F
Average value: 0.728 J/cm Grade Count:1
 0.427 - 0.427 J/cm
@Thickness 1.57 - 1.57 mm
0.800 - 0.800 ft-lb/in
@Thickness 0.0618 - 0.0618 in
Average value: 0.728 J/cm Grade Count:1
Izod Impact, Unnotched 5.34 J/cm - NB10.0 ft-lb/in - NBAverage value: 6.18 J/cm Grade Count:7
Izod Impact, Notched (ISO) 1.57 kJ/m² - NB0.749 ft-lb/in² - NBAverage value: 5.18 kJ/m² Grade Count:27
 2.70 - 6.00 kJ/m²
@Temperature -40.0 - -30.0 °C
1.28 - 2.86 ft-lb/in²
@Temperature -40.0 - -22.0 °F
Average value: 4.37 kJ/m² Grade Count:9
Izod Impact, Unnotched (ISO) 45.0 - 55.0 kJ/m²
@Temperature -30.0 - -30.0 °C
21.4 - 26.2 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 50.0 kJ/m² Grade Count:1
Charpy Impact Unnotched 3.00 J/cm² - NB14.3 ft-lb/in² - NBAverage value: 8.06 J/cm² Grade Count:54
 2.00 J/cm² - NB
@Temperature -40.0 - -20.0 °C
9.52 ft-lb/in² - NB
@Temperature -40.0 - -4.00 °F
Average value: 8.59 J/cm² Grade Count:26
Charpy Impact, Notched 0.150 J/cm² - NB0.714 ft-lb/in² - NBAverage value: 0.740 J/cm² Grade Count:64
 0.150 J/cm² - NB
@Temperature -40.0 - -20.0 °C
0.714 ft-lb/in² - NB
@Temperature -40.0 - -4.00 °F
Average value: 0.404 J/cm² Grade Count:27
Tensile Creep Modulus, 1000 hours 700 MPa102000 psiAverage value: 700 MPa Grade Count:3
Taber Abrasion, mg/1000 Cycles 5.00 - 10.05.00 - 10.0Average value: 7.63 Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 100 - 1.00e+19 ohm-cm100 - 1.00e+19 ohm-cmAverage value: 1.44e+17 ohm-cm Grade Count:85
Surface Resistance 100 - 1.00e+15 ohm100 - 1.00e+15 ohmAverage value: 1.83e+14 ohm Grade Count:42
Dielectric Constant 2.70 - 7.002.70 - 7.00Average value: 3.90 Grade Count:33
Dielectric Strength 10.0 - 70.0 kV/mm254 - 1780 kV/inAverage value: 25.4 kV/mm Grade Count:68
Dissipation Factor 0.00300 - 0.2000.00300 - 0.200Average value: 0.0420 Grade Count:23
Dielectric Loss Index 0.0200 - 0.3000.0200 - 0.300Average value: 0.128 Grade Count:6
Arc Resistance 110 - 180 sec110 - 180 secAverage value: 130 sec Grade Count:12
Comparative Tracking Index 225 - 600 V225 - 600 VAverage value: 572 V Grade Count:61
Hot Wire Ignition, HWI 7.00 - 120 sec7.00 - 120 secAverage value: 59.9 sec Grade Count:9
High Amp Arc Ignition, HAI 15.0 - 120 arcs15.0 - 120 arcsAverage value: 108 arcs Grade Count:10
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min0.000 - 0.394 in/minAverage value: 5.00 mm/min Grade Count:4
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 - 149 µm/m-°C22.2 - 83.0 µin/in-°FAverage value: 72.9 µm/m-°C Grade Count:44
 70.0 - 70.0 µm/m-°C
@Temperature 55.0 - 160 °C
38.9 - 38.9 µin/in-°F
@Temperature 131 - 320 °F
Average value: 62.3 µm/m-°C Grade Count:2
 59.0 - 60.0 µm/m-°C
@Temperature 35.0 - 55.0 °C
32.8 - 33.3 µin/in-°F
@Temperature 95.0 - 131 °F
Average value: 62.3 µm/m-°C Grade Count:3
 59.0 - 60.0 µm/m-°C
@Thickness 2.00 - 2.00 mm
32.8 - 33.3 µin/in-°F
@Thickness 0.0787 - 0.0787 in
Average value: 62.3 µm/m-°C Grade Count:3
CTE, linear, Transverse to Flow 62.0 - 149 µm/m-°C34.4 - 83.0 µin/in-°FAverage value: 81.2 µm/m-°C Grade Count:9
Specific Heat Capacity 2.59 - 2.59 J/g-°C
@Temperature 280 - 280 °C
0.619 - 0.619 BTU/lb-°F
@Temperature 536 - 536 °F
Average value: 2.59 J/g-°C Grade Count:2
Thermal Conductivity 0.245 - 0.370 W/m-K1.70 - 2.57 BTU-in/hr-ft²-°FAverage value: 0.305 W/m-K Grade Count:5
 0.170 - 0.170 W/m-K
@Temperature 280 - 280 °C
1.18 - 1.18 BTU-in/hr-ft²-°F
@Temperature 536 - 536 °F
Average value: 0.170 W/m-K Grade Count:2
Melting Point 221 - 275 °C430 - 527 °FAverage value: 258 °C Grade Count:92
Maximum Service Temperature, Air 80.0 - 220 °C176 - 428 °FAverage value: 126 °C Grade Count:21
Hot Ball Pressure Test 200 - 220 °C392 - 428 °FAverage value: 215 °C Grade Count:4
Deflection Temperature at 0.46 MPa (66 psi) 95.0 - 255 °C203 - 491 °FAverage value: 212 °C Grade Count:89
Deflection Temperature at 1.8 MPa (264 psi) 60.0 - 250 °C140 - 482 °FAverage value: 84.6 °C Grade Count:123
Vicat Softening Point 180 - 250 °C356 - 482 °FAverage value: 227 °C Grade Count:19
Glass Transition Temp, Tg 20.0 - 80.0 °C68.0 - 176 °FAverage value: 50.0 °C Grade Count:3
UL RTI, Electrical 65.0 - 150 °C149 - 302 °FAverage value: 115 °C Grade Count:16
UL RTI, Mechanical with Impact 65.0 - 110 °C149 - 230 °FAverage value: 78.4 °C Grade Count:15
UL RTI, Mechanical without Impact 65.0 - 130 °C149 - 266 °FAverage value: 99.4 °C Grade Count:16
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:124
Oxygen Index 22.0 - 39.0 %22.0 - 39.0 %Average value: 32.5 % Grade Count:32
Glow Wire Test 700 - 960 °C1290 - 1760 °FAverage value: 913 °C Grade Count:35
 
Processing PropertiesMetricEnglishComments
Processing Temperature 235 - 310 °C455 - 590 °FAverage value: 280 °C Grade Count:13
Nozzle Temperature 250 - 293 °C482 - 560 °FAverage value: 272 °C Grade Count:19
Melt Temperature 220 - 305 °C428 - 581 °FAverage value: 273 °C Grade Count:65
Mold Temperature 40.0 - 107 °C104 - 225 °FAverage value: 75.5 °C Grade Count:61
Drying Temperature 71.1 - 130 °C160 - 266 °FAverage value: 85.6 °C Grade Count:52
Moisture Content 0.0300 - 0.200 %0.0300 - 0.200 %Average value: 0.183 % Grade Count:24
Dew Point -40.0 - -17.8 °C-40.0 - 0.000 °FAverage value: -24.4 °C Grade Count:5
Injection Pressure 4.96 - 138 MPa720 - 20000 psiAverage value: 74.7 MPa Grade Count:15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, Unreinforced
Overview of materials for Nylon 66, Impact Grade
Overview of materials for Nylon 66/6
Overview of materials for Nylon 66, 10% Glass Fiber Filled
Overview of materials for Nylon 66, Heat Stabilized

O2502 / 78001

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.