Daikin PTFE F-201 is a polytetrafluoroethylene fine powder resin for paste extrusion manufactured without the use of PFOA. F-201 has been designed for spaghetti tubing, thin wall tubing and wire coating applications of less than 16 AWG that are run at high reduction ratios.Information provided by Daikin. |