MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled
Categories: Polymer; Thermoset; Diallyl Phthalate (DAP); Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.72 - 1.82 g/cc0.0621 - 0.0658 lb/in³Average value: 1.78 g/cc Grade Count:18
Water Absorption 0.250 - 0.350 %0.250 - 0.350 %Average value: 0.280 % Grade Count:12
 0.250 - 0.300 %
@Temperature 50.0 - 50.0 °C
0.250 - 0.300 %
@Temperature 122 - 122 °F
Average value: 0.275 % Grade Count:4
 0.250 - 0.300 %
@Time 173000 - 173000 sec
0.250 - 0.300 %
@Time 48.0 - 48.0 hour
Average value: 0.275 % Grade Count:4
Linear Mold Shrinkage 0.00100 - 0.00400 cm/cm0.00100 - 0.00400 in/inAverage value: 0.00250 cm/cm Grade Count:18
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 41.0 - 88.0 MPa5950 - 12800 psiAverage value: 58.7 MPa Grade Count:17
Flexural Yield Strength 89.6 - 143 MPa13000 - 20700 psiAverage value: 110 MPa Grade Count:18
Flexural Modulus 13.8 - 20.0 GPa2000 - 2900 ksiAverage value: 15.9 GPa Grade Count:6
Compressive Yield Strength 140 - 207 MPa20300 - 30000 psiAverage value: 177 MPa Grade Count:17
Izod Impact, Notched 0.520 - 3.50 J/cm0.974 - 6.56 ft-lb/inAverage value: 2.19 J/cm Grade Count:18
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+16 - 1.00e+17 ohm-cm1.00e+16 - 1.00e+17 ohm-cmAverage value: 7.00e+16 ohm-cm Grade Count:12
 2.00e+10 - 5.00e+10 ohm-cm
@Temperature 70.0 - 70.0 °C
2.00e+10 - 5.00e+10 ohm-cm
@Temperature 158 - 158 °F
Average value: 3.25e+10 ohm-cm Grade Count:4
 2.00e+10 - 5.00e+10 ohm-cm
@Time 2.59e+6 - 2.59e+6 sec
2.00e+10 - 5.00e+10 ohm-cm
@Time 720 - 720 hour
Average value: 3.25e+10 ohm-cm Grade Count:4
Surface Resistance 1.00e+16 - 1.00e+17 ohm1.00e+16 - 1.00e+17 ohmAverage value: 7.00e+16 ohm Grade Count:12
 2.60e+10 - 5.00e+10 ohm
@Temperature 70.0 - 70.0 °C
2.60e+10 - 5.00e+10 ohm
@Temperature 158 - 158 °F
Average value: 4.40e+10 ohm Grade Count:4
 2.60e+10 - 5.00e+10 ohm
@Time 2.59e+6 - 2.59e+6 sec
2.60e+10 - 5.00e+10 ohm
@Time 720 - 720 hour
Average value: 4.40e+10 ohm Grade Count:4
Dielectric Constant 3.50 - 40.03.50 - 40.0Average value: 4.96 Grade Count:17
Dielectric Strength 13.4 - 18.7 kV/mm340 - 475 kV/inAverage value: 15.4 kV/mm Grade Count:18
Dielectric Breakdown 60.0 - 64.0 V60.0 - 64.0 VAverage value: 61.5 V Grade Count:4
Dissipation Factor 0.00600 - 0.01900.00600 - 0.0190Average value: 0.0120 Grade Count:17
Arc Resistance 130 - 180 sec130 - 180 secAverage value: 165 sec Grade Count:18
Comparative Tracking Index 600 V600 VAverage value: 600 V Grade Count:4
 
Thermal PropertiesMetricEnglishComments
CTE, linear 15.0 - 24.0 µm/m-°C8.33 - 13.3 µin/in-°FAverage value: 22.6 µm/m-°C Grade Count:17
Maximum Service Temperature, Air 130 °C266 °FAverage value: 130 °C Grade Count:5
Deflection Temperature at 1.8 MPa (264 psi) 260 - 280 °C500 - 536 °FAverage value: 261 °C Grade Count:14
Heat Distortion Temperature 260 °C500 °FAverage value: 260 °C Grade Count:4
Flammability, UL94 V-0V-0Grade Count:8
Oxygen Index 30.0 - 41.0 %30.0 - 41.0 %Average value: 35.2 % Grade Count:6
 
Processing PropertiesMetricEnglishComments
Processing Temperature 135 - 165 °C275 - 329 °FAverage value: 150 °C Grade Count:8
Mold Temperature 135 - 190 °C275 - 374 °FAverage value: 158 °C Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
Overview of materials for Phenolic; Unreinforced; Molded

O1531 / 77881

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.