MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ITW Insulcast® RTVS 61M Silicone Potting/Encapsulation Compound
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Encapsulation Grade

Material Notes: Insulcast® solutions are compounds designed for potting and encapsulating. RTVS 61M is a low viscosity, self-extinguishing transparent RTVS Silicone. RTVS 61M is used in situations where component identification and protection against shock and vibration is needed. Heat can be used to accelerate the cure.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/ccUncured. Part A
 1.00 g/cc1.00 g/ccUncured. Part B
 1.02 g/cc1.02 g/ccUncured. Mixed. Part A, Part B
Viscosity 4000 cP4000 cPPart A; ASTM D1084
 4500 cP4500 cPMixed, Part A, Part B; ASTM D1084
 5000 cP5000 cPPart B; ASTM D1084
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3535ASTM D2240
Tensile Strength 2.76 MPa400 psiASTM D412
Elongation at Break 150 %150 %ASTM D412
Tear Strength 4.38 kN/m25.0 pliDie B; ASTM D624
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Constant 2.7
@Frequency 1000 Hz
2.7
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 19.7 kV/mm500 kV/inASTM D149
Dissipation Factor 0.0010
@Frequency 1000 Hz
0.0010
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 270 µm/m-°C150 µin/in-°F
Thermal Conductivity 0.0159 W/m-K0.110 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Shrinkage 0.20 %0.20 %
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 min
@Temperature 95.0 °C
1.00 hour
@Temperature 203 °F
option
 120 min
@Temperature 50.0 °C
2.00 hour
@Temperature 122 °F
option
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
option
Pot Life 120 min120 minPart A, Part B
Shelf Life 6.00 Month6.00 MonthPart A, Part B
 
Descriptive Properties
Colorclearpart A, uncured
 clearpart B, uncured
Mix Ratio by weight10:1Part A: Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWIN9124 / 239634

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.