MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akro-Plastic Akrotek® PEEK TM black (5051) PEEK, Conditioned
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: Description: AKROTEK® PEEK TM black (5051) is an unreinforced polyetheretherketone with good tribological properties

Applications: Applications are mainly elements in the automotive-, aeronautical-, industrial- and medical engineering that require low friction and wear values in a temperature environment above 150 °C

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³ISO 1183
 
Thermal PropertiesMetricEnglishComments
Melting Point 342 °C648 °FDSC, 10K/min; DIN EN 11357-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
Akro-Plastic Akrotek® PEEK GF 50 natural (5100) PEEK, Conditioned, 50% Glass Filled
Akro-Plastic Akrotek® PEEK GF 50 natural (5100) PEEK, Dry, 50% Glass Filled
Akro-Plastic Akrotek® PEEK GF 60 9 natural (5184) PEEK, Conditioned, 60% Glass Filled
Akro-Plastic Akrotek® PEEK natural (5184) PEEK, Dry

PAKRO445 / 183032

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.