MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Saint-Gobain Chemfab® 313XK PTFE Coated Fiberglass/Kevlar Conveyor Belting
Categories: Ceramic; Glass; Glass Fiber

Material Notes: Description: General Notes on Saint Gobain Belting Products:
Saint Gobain Performance Plastics developed its belting materials for applications that require superior release characteristics, permeability for rapid drying, dimensional and thermal stability, and the dynamic strength to stand up to the most rigorous operating conditions. The unique behavior of the materials results in a product that is more practical and cost-effective than conventional belting materials.
Release Properties: The release characteristics of PTFE are superior to those of any other high-temperature material. This non-stick property is retained over a full range of operating temperatures.
Permeability: Our belting combines a maximum amount of open area with good mechanical strength. The result is a very high level of controlled air flow through the belt, maximizing the rate of drying.
Dimensional Stability: The woven reinforcement results in an elongation of approximately 1% under normal mechanical loading, even at temperatures of 550°F. Length distortion is exceptionally low, while width rigidity and stability are enhanced by the high modulus of the reinforcement.
Thermal Stability: Chemfab® brand belting may be used continuously at temperatures up to 550°F without reducing its performance.
Dynamic Stability: Our belting has been subjected to static and dynamic tests which indicate that it can withstand all normal operating conditions affecting service life.
Chemical Resistance: PTFE surfaces are unaffected by most chemicals and solvents.

Notes on 313XK PTFE Coated Fiberglass/Kevlar Conveyor Belting:
Chemfab® 313XK is a belting product used in applications that require high strength and low elongation. This material has inherent stability that enhances its ability to resist ridging, puckering and creasing. The surface is textured because of the use of large yarns in the fiberglass substrate. The addition of Kevlar® in the warp gives added strength in terms of both tensile and tears, and also provides excellent flex fatigue resistance and moisture resistance. The substrate is fiberglass/Kevlar and the coating material is PTFE (PTFE = polytetrafluoroethylene). All data based on a 0.03 inch test sample.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.557 g/cc0.05626 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Elongation at Yield <= 1.0 %<= 1.0 %Value given for Elongation at a loading of 40 lbs/in
Tear Strength Test 4545Lbs./In. Propagation Tear Strength in fill/transverse direction
 130130Lbs./In. for warp/longitudinal Propagation Tear Strength
Tear Strength 96.4 kN/m550 pliTensile Strength (Fill)
 158 kN/m900 pliTensile Strength (Warp)
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 288 °C550 °F
 
Descriptive Properties
Weight (oz/yd^2)35

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SpinTech Veritex™ Shape Memory Polymer Composite
Arlon Electronic Materials 45NK Woven Kevlar® Reinforced Laminate and Prepreg
Global EPP PA 6E Extruded Polyamide 6
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm
Firestone C200-001 Nylon 6

CSTGQZ111 / 2240

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.