MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

AK Steel 12 SR™ Ferritic Stainless steel  (discontinued **)
Categories: Metal; Ferrous Metal; Ferritic; Stainless Steel

Material Notes: AK Steel 12 SR™ provides a more oxidation-resistant alternative to Type 409 stainless steel. In addition it provides formability and weldability comparable to other more highly alloyed ferritic stainless steels. AK Steel 12 SR™ was developed specifically for automotive exhaust gas applications. Non-automotive applications include heat exchangers, flue liners, and commercial furnaces.

Mechanical properties for 1950°F Anneal

Information provided by AK Steel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.63 g/cc0.276 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 80.580.5Typical
 <= 92<= 92Specification
Tensile Strength, Ultimate >= 448 MPa>= 65000 psiSpecification
 503 MPa73000 psiTypical
 35.0 MPa
@Temperature 871 °C
5080 psi
@Temperature 1600 °F
 149 MPa
@Temperature 704 °C
21600 psi
@Temperature 1300 °F
 368 MPa
@Temperature 538 °C
53400 psi
@Temperature 1000 °F
Tensile Strength, Yield  >= 276 MPa
@Strain 0.2 %
>= 40000 psi
@Strain 0.2 %
Specification
 345 MPa
@Strain 0.2 %
50000 psi
@Strain 0.2 %
Typical
 29.0 MPa
@Strain 0.2 %,
Temperature 1600 °C
4210 psi
@Strain 0.2 %,
Temperature 2910 °F
 111 MPa
@Strain 0.2 %,
Temperature 1300 °C
16100 psi
@Strain 0.2 %,
Temperature 2370 °F
 196 MPa
@Strain 0.2 %,
Temperature 1000 °C
28400 psi
@Strain 0.2 %,
Temperature 1830 °F
Elongation at Break >= 20 %>= 20 %in 2 inches, Specification
 31.5 %31.5 %in 2 inches, Typical
Modulus of Elasticity 189 GPa27400 ksi
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 1.2 %1.2 %
Carbon, C 0.020 %0.020 %
Chromium, Cr 12 %12 %
Iron, Fe 85.38 %85.38 %As Remainder
Niobium, Nb (Columbium, Cb) 0.60 %0.60 %
Silicon, Si 0.50 %0.50 %
Titanium, Ti 0.30 %0.30 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum AL 409HP™ Ferritic Stainless Steel, UNS S40930
Schwarzkopf Plansee PM 2000, Sheet Grain Class 6 ODS Iron Alloy Sheet
AISI 1020 Steel, cold rolled
AISI Grade 18Ni (200) Maraging Steel, Annealed
Alliance N-33 Neodymium Iron Boron Magnetic Material

NAKS089 / 14692

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.