MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Momentive Performance Materials FPD Boron Nitride (BN) Coating  (discontinued **)
Categories: Ceramic; Nitride; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Can be applied by brush, roller, dipping, or spraying. Can be applied to either hot or cold services although use of water based coatings on surfaces greater than 100°C is not recommended. Multiple coats may be necessary. Dried coatings can be readily handled, smoothed, or polished with a soft, dry cloth.

Uses of Advanced Ceramics Corporation boron nitride water based coatings and aerosol spray:

Release Agents, Lubricants and Protective Coatings Boron Nitride (BN) remains lubricious and inert even at extremely high temperatures. Coatings made with BN prevent sticking to increase the life of dies/molds, improve product surface finishes, and reduce production times.

Metalforming In molten metal and metalforming applications, BN coatings protect surfaces which come in contact with hot and molten metals. BN inhibits corrosion and chemical attack and provides easier release and longer mold/die life. Applications include: casting, stamping, forging and powder metallurgy.

Glass Making BN's high temperature lubricating properties make it ideal in glass making where it helps minimize surface defects, improve mold/die life and release, and reduce clean-up time. Most glass formulations will not stick to BN.

Plastics/Rubber Producers of injection-molded plastics and elastomers benefit from BN die applications by improved die release and increased production speeds.

Sintering Sintering of metallic and ceramic powders is typically done on graphite plates. A coating of BN can essentially eliminate carbon contamination, reactivity and sticking which can occur at sintering temperatures.

Welding and Brazing BN coatings are also ideal for welding and furnace brazing. They protect surfaces from weld spatter and provide superior stop-off protection. BN coatings also protect MIG/MAG welding nozzles from weld spatter.

Information provided by GE Advanced Ceramics.

Information provided by Momentive Performance Materials, formerly GE Advanced Ceramics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmtypical (Boron Nitride Component)
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 850 °C1560 °FOxidizing
Maximum Service Temperature, Inert 1800 °C3270 °FInert/Vacuum
 
Descriptive Properties
ApplicationRelease, Forging Lubrication
ColorWhite
Contents BinderBN/Alumina Bentonite
DilutionPer Instructions
Relative Hardness2On a scale of 1-4 with 1 being the hardest.
Solvent TypeDry

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Water, H2O
Boron Nitride, Cubic BN, (Borazone)
Momentive Performance Materials HPC Boron Nitride (BN)/TiO2 Water Based Coating
Titanium Nitride (TiN) Coating
Boron Nitride, 60% SiO2 - 40% BN

CADV07 / 399

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.