MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Dow Dow™ 748I LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Product Description: A low density polyethylene for stretching/clip film applications
Complies with: US FDA 21 CFR 177.1520©2.1; Canadian HPFB No Objection (with Limitations). Consult the regulations for complete details.

Availability: Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520©2.1; Canadian HPFB No Objection

Form: Pellets

Processing Method: Blown Film

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³ASTM D792
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 10.6 MPa
@Thickness 0.0254 mm
1540 psi
@Thickness 0.00100 in
ASTM D882
Film Tensile Strength at Yield, TD 10.0 MPa
@Thickness 0.0254 mm
1450 psi
@Thickness 0.00100 in
ASTM D882
Film Elongation at Break, MD 510 %
@Thickness 0.0254 mm
510 %
@Thickness 0.00100 in
ASTM D882
Film Elongation at Break, TD 640 %
@Thickness 0.0254 mm
640 %
@Thickness 0.00100 in
ASTM D882
Elmendorf Tear Strength MD 190 g
@Thickness 0.0254 mm
190 g
@Thickness 0.00100 in
ASTM D1922
Elmendorf Tear Strength TD 260 g
@Thickness 0.0254 mm
260 g
@Thickness 0.00100 in
ASTM D1922
Dart Drop Test 43.0 g
@Thickness 0.0254 mm
0.0948 lb
@Thickness 0.00100 in
ASTM D1709A
Film Tensile Strength at Break, MD 27.1 MPa
@Thickness 0.0254 mm
3930 psi
@Thickness 0.00100 in
ASTM D882
Film Tensile Strength at Break, TD 17.5 MPa
@Thickness 0.0254 mm
2540 psi
@Thickness 0.00100 in
ASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 110 °C230 °F
Vicat Softening Point 88.9 °C192 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 1.1 %
@Thickness 0.0254 mm
1.1 %
@Thickness 0.00100 in
ASTM D1003
Gloss 92 %
@Thickness 0.0254 mm
92 %
@Thickness 0.00100 in
45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °FExtrusion
 
Descriptive Properties
Film Puncture Resistance32 ft-lb/in32.0 mil
Film Toughness1880 ft-lb/in3TD, 1.0 mil, ASTM D882
 2220 ft-lb/in3MD, 1.0 mil, ASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF474 / 311167

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.