MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

GEHR Plastics POM-C 25GF®
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, 30% Glass Fiber Reinforced

Material Notes: The chemically coupled GEHR-C POM 25GFTM has a broad property profile that offers increased strength for many applications compared to non-reinforced GEHR POM™. In addition, the reinforcement reduces the coefficient of expansion and simultaneously increases the heat deflection temperature.

Features: Pressure tested quality; High strength and stiffness; High rigidity (to -40 °C); High thermal stability; Low water absorption; High dimension stability; Good electrical insulating properties; Very good sliding properties; High resistance to solvents; Very high resistance to stress cracks

Applications: Components in machinery engineering

Information provided by GEHR Plastics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.58 g/cc1.58 g/ccISO 1183
Water Absorption 0.900 %0.900 %ISO 62
Moisture Absorption 0.150 %0.150 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell H 190190ISO 2039
Tensile Strength at Break 130 MPa18900 psiISO 527
Elongation at Break 3.00 %3.00 %ISO 527
Modulus of Elasticity 8.80 GPa1280 ksiISO 527
Charpy Impact Unnotched 5.50 J/cm²26.2 ft-lb/in²ISO 179
Charpy Impact, Notched 0.800 J/cm²3.81 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+12 ohm-cm>= 1.00e+12 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmIEC 60093
Dielectric Constant 4.00
@Frequency 1.00e+6 Hz
4.00
@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 43.0 kV/mm1090 kV/inIEC 60243-1
Dielectric Loss Index 0.00700
@Frequency 1.00e+6 Hz
0.00700
@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 168 °C334 °FISO 3146
Maximum Service Temperature, Air 110 °C230 °FUL746B
Deflection Temperature at 1.8 MPa (264 psi) 163 °C325 °FISO 75
Vicat Softening Point 160 °C320 °FVST/B/50; ISO 306
Minimum Service Temperature, Air -40.0 °C-40.0 °FUL746B
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGEHR104 / 327197

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.