MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem HDP0353 High density polyethylene copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: HDP0353 is a high density polyethylene copolymer developed for solid wall and corrugated piping applications. Industrial Standard Compliance ASTM D3350: Cell Classification PE 435620A. The resin HDP0353 meet the material requirements specifications ASTM F2160. This resin is recommended for use in applications that are required to meet AASHTO M294 specifications.
Applications: Natural bimodal high density polyethylene copolymer , resin designed for solid wall and corrugated pipes of small and large diameter, and telecommunications conduits.
Processes: Pipes extrusion.

Test specimens from compression molded plaque according to ASTM D4703.

Information provided by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.953 g/cc0.0344 lb/in³ASTM D792
ESCR 100% Igepal® >= 1500 hour>= 1500 hourCondition B; ASTM D1693
ESCR 10% Igepal® >= 1500 hour>= 1500 hourCondition B; ASTM D1693
Oxidative Induction Time (OIT) 45 min
@Temperature 200 °C
45 min
@Temperature 392 °F
ASTM D3895
Melt Flow 0.35 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ASTM D2240
Tensile Strength at Break 38.0 MPa5510 psiASTM D638
Tensile Strength, Yield 26.0 MPa3770 psiASTM D638
Elongation at Break 665 %665 %ASTM D638
Flexural Modulus, 1% Secant 1275 MPa184900 psiASTM D790
Izod Impact, Unnotched 1.65 J/cm3.09 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C158 °FASTM D648
Vicat Softening Point 125 °C
@Load 1.02 kg
257 °F
@Load 2.25 lb
ASTM D1525
Brittleness Temperature <= -75.0 °C<= -103 °FASTM D1693

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBRAS622 / 314015

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.