MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Azoty Tarnow™ TARNOFORM 300 MW4 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Mineral Filled

Material Notes: Mineral filled injection molding grade based on Tarnoform 300 reinforced with 20% wollastonite; such a compound has high stiffness, dimensional stability and hardness combined with low shrinkage.

Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.54 g/cc0.0556 lb/in³ISO 1183
Linear Mold Shrinkage 0.0122 cm/cm0.0122 in/in60x60x4
Linear Mold Shrinkage, Transverse 0.0215 cm/cm0.0215 in/inISO 294-4
Melt Flow 6.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
6.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ISO 2039-2
Ball Indentation Hardness 160 MPa23200 psi358 N; ISO 2039-1
Tensile Strength, Yield 73.0 MPa10600 psiISO 527
Elongation at Break 2.5 %2.5 %ISO 527
Flexural Strength 106 MPa15400 psiISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²1.43 ft-lb/in²1A; ISO 180
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²1eA; ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Constant 4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 112
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.30 J/g-°C0.311 BTU/lb-°F
Melting Point 170 °C338 °F10°C/min.; ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 148 °C298 °FISO 75
Vicat Softening Point 158 °C316 °F50 N; ISO 306
Flammability, UL94 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 230 °C356 - 446 °FBarrel temperature
Mold Temperature 60.0 - 120 °C140 - 248 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PZAK026 / 72865

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.