MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

United Cast Bar Unibar 700-2 Continuously Cast Spheroidal Graphite Iron
Categories: Metal; Ferrous Metal; Cast Iron; Gray Cast Iron

Material Notes: Offers higher wear resistance; strength & heat-treatment response while still possessing reasonable machinability and excellent surface finish. Noise and vibration damping are good in this grade.

Unibar 700-2 can be hardened by conventional methods, to Rc 50 on the bar surface, responds well to austempering (ADI).

Information provided by United Cast Bar Ltd.

Key Words: EN-1563-GJS-700-2 GGG70; Meehanite SP700.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.30 g/cc0.264 lb/inĀ³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 230 - 305
@Load 3000 kg
230 - 305
@Load 6610 lb
10 mm ball
Tensile Strength  660 MPa
@Diameter 105 - 200 mm
95700 psi
@Diameter 4.13 - 7.87 in
 660 MPa
@Diameter 205 - 600 mm
95700 psi
@Diameter 8.07 - 23.6 in
 700 MPa
@Diameter 25.0 - 50.0 mm
102000 psi
@Diameter 0.984 - 1.97 in
 700 MPa
@Diameter 55.0 - 100 mm
102000 psi
@Diameter 2.17 - 3.94 in
Tensile Strength, Yield  380 MPa
@Diameter 105 - 200 mm,
Strain 0.2 %
55100 psi
@Diameter 4.13 - 7.87 in,
Strain 0.2 %
 380 MPa
@Diameter 205 - 600 mm,
Strain 0.2 %
55100 psi
@Diameter 8.07 - 23.6 in,
Strain 0.2 %
 400 MPa
@Diameter 55.0 - 100 mm,
Strain 0.2 %
58000 psi
@Diameter 2.17 - 3.94 in,
Strain 0.2 %
 420 MPa
@Diameter 25.0 - 50.0 mm,
Strain 0.2 %
60900 psi
@Diameter 0.984 - 1.97 in,
Strain 0.2 %
Elongation at Break  1.0 %
@Thickness 105 - 200 mm
1.0 %
@Thickness 4.13 - 7.87 in
 1.0 %
@Thickness 205 - 600 mm
1.0 %
@Thickness 8.07 - 23.6 in
 2.0 %
@Thickness 25.0 - 50.0 mm
2.0 %
@Thickness 0.984 - 1.97 in
 2.0 %
@Thickness 55.0 - 100 mm
2.0 %
@Thickness 2.17 - 3.94 in
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 3.25 - 3.7 %3.25 - 3.7 %
Iron, Fe 92.83 - 94.19 %92.83 - 94.19 %as balance
Magnesium, Mg 0.040 - 0.070 %0.040 - 0.070 %
Manganese, Mn 0.10 - 0.30 %0.10 - 0.30 %
Phosphorus, P 0.015 - 0.080 %0.015 - 0.080 %
Silicon, Si 2.4 - 3.0 %2.4 - 3.0 %
Sulfur, S 0.0050 - 0.020 %0.0050 - 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron
United Cast Bar Unibar 500-7 Continuously Cast Spheroidal Graphite Iron
United Cast Bar Unibar 400-15 As Cast Continuously Cast Spheroidal Graphite Iron
United Cast Bar Unibar 600-3 Continuously Cast Spheroidal Graphite Iron
Ductile Iron grade 60-40-18

NUNITED09 / 160456

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.