MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ascend Performance Materials Vydyne® STAT B 30 FC BK PA6-CF30
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Carbon Fiber Filled

Material Notes: Vydyne STAT B 30 FC BK is standard flow 30% carbon-fiber reinforced PA6 resin. Available in black, it is specifically designed for high stiffness and strength. This product is also electrically conductive.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³DAM; ISO 1183
Moisture Absorption at Equilibrium 2.1 %2.1 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm
@Thickness 2.00 mm
0.0020 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
@Thickness 2.00 mm
0.0050 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 160 MPa23200 psi50% RH; ISO 527-2
 210 MPa30500 psiDAM; ISO 527-2
Elongation at Break 1.5 %1.5 %DAM; ISO 527-2
 3.5 %3.5 %50% RH; ISO 527-2
Tensile Modulus 13.0 GPa1890 ksi50% RH; ISO 527-2
 18.5 GPa2680 ksiDAM; ISO 527-2
Charpy Impact Unnotched 8.50 J/cm²
@Temperature 23.0 °C
40.4 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10000 ohm-cm
@Thickness 1.00 mm
10000 ohm-cm
@Thickness 0.0394 in
DAM; IEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °C419 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FUnannealed; DAM; ISO 75-2/A
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 270 °C446 - 518 °FInjection
Middle Barrel Temperature 230 - 275 °C446 - 527 °FInjection
Front Barrel Temperature 230 - 275 °C446 - 527 °FInjection
Nozzle Temperature 230 - 275 °C446 - 527 °FInjection
Melt Temperature 230 - 275 °C446 - 527 °FInjection
Mold Temperature 80.0 - 90.0 °C176 - 194 °FInjection
Drying Temperature 80.0 - 100 °C176 - 212 °FInjection
Dry Time >= 3.00 hour>= 3.00 hourInjection
 
Descriptive Properties
AdditiveLubricant
AppearanceBlack
FeaturesChemical Resistant
 Gasoline Resistant
 General Purpose
 Good Dimensional Stability
 Good Flow
 Good Stiffness
 High Tensile Strength
 Lubricated
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE9368 / 287659

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.