Beijing Evergrow Resources PTFE Tube and Pipe
Categories:
Polymer
;
Thermoplastic
;
Fluoropolymer
;
Polytetrafluoroethylene (PTFE)
;
Polytetrafluoroethylene (PTFE), Extruded
Material Notes:
PTFE tubing is manufactured by ram extruding method with PTFE granular resin. It has good electrical properties.
Information provided by Beijing Evergrow Resources.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
2.10
-
2.30
g/cc
0.0759
-
0.0831
lb/in³
apparent
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
>=
18.0
MPa
>=
2610
psi
Elongation at Break
>= 230 %
>= 230 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Beijing Evergrow Resources PTFE Extrusion Tube
Beijing Evergrow Resources PTFE Sheet
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
DuPont Mobility and Materials Kalrez® 4079 FFKM Perfluoroelastomer
Chemours Viton® F-605C Fluoroelastomer (FKM)
PBEIJ029 / 90098
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.