Physical Properties | Metric | English | Comments |
---|
Density | 1.40 g/cc | 0.0506 lb/in³ |
Water Absorption | 1.2 % @Temperature 23.0 °C, Time 86400 sec | 1.2 % @Temperature 73.4 °F, Time 24.0 hour |
Moisture Absorption at Equilibrium | 1.9 % | 1.9 % |
Linear Mold Shrinkage, Flow | 0.0030 cm/cm @Thickness 2.00 mm | 0.0030 in/in @Thickness 0.0787 in |
Linear Mold Shrinkage, Transverse | 0.011 cm/cm @Thickness 2.00 mm | 0.011 in/in @Thickness 0.0787 in |
|
Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength at Break | 91.0 MPa | 13200 psi |
| 127 MPa | 18400 psi |
Elongation at Break | 2.7 % | 2.7 % |
| 3.0 % | 3.0 % |
Tensile Modulus | 6.90 GPa | 1000 ksi |
| 8.50 GPa | 1230 ksi |
Flexural Strength | 127 MPa | 18400 psi |
| 193 MPa | 28000 psi |
Flexural Modulus | 5.90 GPa | 856 ksi |
| 9.10 GPa | 1320 ksi |
Izod Impact, Notched (ISO) | 7.70 kJ/m² @Temperature -40.0 °C | 3.66 ft-lb/in² @Temperature -40.0 °F |
| 7.70 kJ/m² @Temperature -40.0 °C | 3.66 ft-lb/in² @Temperature -40.0 °F |
| 7.80 kJ/m² @Temperature -30.0 °C | 3.71 ft-lb/in² @Temperature -22.0 °F |
| 7.90 kJ/m² @Temperature -30.0 °C | 3.76 ft-lb/in² @Temperature -22.0 °F |
| 8.10 kJ/m² @Temperature 23.0 °C | 3.85 ft-lb/in² @Temperature 73.4 °F |
| 10.0 kJ/m² @Temperature 23.0 °C | 4.76 ft-lb/in² @Temperature 73.4 °F |
Charpy Impact Unnotched | 5.30 J/cm² @Temperature -40.0 °C | 25.2 ft-lb/in² @Temperature -40.0 °F |
| 5.30 J/cm² @Temperature -30.0 °C | 25.2 ft-lb/in² @Temperature -22.0 °F |
| 5.50 J/cm² @Temperature -40.0 °C | 26.2 ft-lb/in² @Temperature -40.0 °F |
| 5.70 J/cm² @Temperature -30.0 °C | 27.1 ft-lb/in² @Temperature -22.0 °F |
| 5.70 J/cm² @Temperature 23.0 °C | 27.1 ft-lb/in² @Temperature 73.4 °F |
| 6.20 J/cm² @Temperature 23.0 °C | 29.5 ft-lb/in² @Temperature 73.4 °F |
Charpy Impact, Notched | 0.760 J/cm² @Temperature -30.0 °C | 3.62 ft-lb/in² @Temperature -22.0 °F |
| 0.790 J/cm² @Temperature -40.0 °C | 3.76 ft-lb/in² @Temperature -40.0 °F |
| 0.830 J/cm² @Temperature -40.0 °C | 3.95 ft-lb/in² @Temperature -40.0 °F |
| 0.830 J/cm² @Temperature -30.0 °C | 3.95 ft-lb/in² @Temperature -22.0 °F |
| 0.890 J/cm² @Temperature 23.0 °C | 4.24 ft-lb/in² @Temperature 73.4 °F |
| 1.10 J/cm² @Temperature 23.0 °C | 5.23 ft-lb/in² @Temperature 73.4 °F |
|
Electrical Properties | Metric | English | Comments |
---|
Dielectric Strength | 42.0 kV/mm @Thickness 1.00 mm | 1070 kV/in @Thickness 0.0394 in |
Comparative Tracking Index | 600 V @Thickness 3.00 mm | 600 V @Thickness 0.118 in |
Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 0.400 mm | 30 - 60 sec @Thickness 0.0157 in |
| 60 - 120 sec @Thickness 0.750 mm | 60 - 120 sec @Thickness 0.0295 in |
| >= 120 sec @Thickness 1.50 mm | >= 120 sec @Thickness 0.0591 in |
| >= 120 sec @Thickness 3.00 mm | >= 120 sec @Thickness 0.118 in |
High Amp Arc Ignition, HAI | >= 120 arcs @Thickness 0.400 mm | >= 120 arcs @Thickness 0.0157 in |
| >= 120 arcs @Thickness 0.750 mm | >= 120 arcs @Thickness 0.0295 in |
| >= 120 arcs @Thickness 1.50 mm | >= 120 arcs @Thickness 0.0591 in |
| >= 120 arcs @Thickness 3.00 mm | >= 120 arcs @Thickness 0.118 in |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear, Parallel to Flow | 23.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C | 12.8 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
CTE, linear, Transverse to Flow | 67.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C | 37.2 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
Melting Point | 260 °C | 500 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 254 °C | 489 °F |
| 256 °C | 493 °F |
Deflection Temperature at 1.8 MPa (264 psi) | 228 °C | 442 °F |
| 237 °C | 459 °F |
UL RTI, Electrical | 140 °C @Thickness 0.200 mm | 284 °F @Thickness 0.00787 in |
| 140 °C @Thickness 0.400 mm | 284 °F @Thickness 0.0157 in |
| 140 °C @Thickness 0.750 mm | 284 °F @Thickness 0.0295 in |
| 140 °C @Thickness 1.50 mm | 284 °F @Thickness 0.0591 in |
| 140 °C @Thickness 3.00 mm | 284 °F @Thickness 0.118 in |
UL RTI, Mechanical with Impact | 95.0 °C @Thickness 0.200 mm | 203 °F @Thickness 0.00787 in |
| 110 °C @Thickness 0.400 mm | 230 °F @Thickness 0.0157 in |
| 120 °C @Thickness 0.750 mm | 248 °F @Thickness 0.0295 in |
| 130 °C @Thickness 1.50 mm | 266 °F @Thickness 0.0591 in |
| 130 °C @Thickness 3.00 mm | 266 °F @Thickness 0.118 in |
UL RTI, Mechanical without Impact | 115 °C @Thickness 0.200 mm | 239 °F @Thickness 0.00787 in |
| 130 °C @Thickness 0.400 mm | 266 °F @Thickness 0.0157 in |
| 140 °C @Thickness 0.750 mm | 284 °F @Thickness 0.0295 in |
| 150 °C @Thickness 1.50 mm | 302 °F @Thickness 0.0591 in |
| 150 °C @Thickness 3.00 mm | 302 °F @Thickness 0.118 in |
Flammability, UL94 | V-0 @Thickness 0.200 mm | V-0 @Thickness 0.00787 in |
| V-0 @Thickness 0.400 mm | V-0 @Thickness 0.0157 in |
| V-0 @Thickness 0.750 mm | V-0 @Thickness 0.0295 in |
| V-0 @Thickness 1.50 mm | V-0 @Thickness 0.0591 in |
| V-0 @Thickness 3.00 mm | V-0 @Thickness 0.118 in |
| 5VA @Thickness 1.50 mm | 5VA @Thickness 0.0591 in |
| 5VA @Thickness 3.00 mm | 5VA @Thickness 0.118 in |
Glow Wire Flammability Index | 960 °C @Thickness 0.200 mm | 1760 °F @Thickness 0.00787 in |
| 960 °C @Thickness 0.400 mm | 1760 °F @Thickness 0.0157 in |
| 960 °C @Thickness 0.750 mm | 1760 °F @Thickness 0.0295 in |
| 960 °C @Thickness 1.50 mm | 1760 °F @Thickness 0.0591 in |
| 960 °C @Thickness 3.00 mm | 1760 °F @Thickness 0.118 in |
|
Processing Properties | Metric | English | Comments |
---|
Rear Barrel Temperature | 275 - 300 °C | 527 - 572 °F |
Middle Barrel Temperature | 275 - 300 °C | 527 - 572 °F |
Front Barrel Temperature | 275 - 300 °C | 527 - 572 °F |
Melt Temperature | 275 - 300 °C | 527 - 572 °F |
Mold Temperature | 60.0 - 120 °C | 140 - 248 °F |
Drying Temperature | 80.0 °C | 176 °F |
Dry Time | 4.00 - 6.00 hour | 4.00 - 6.00 hour |
|
Descriptive Properties |
---|
Additive | Flame Retarding Agent |
Appearance | Black |
Automotive Material Specification | Tesla TM-1006-303120V (compliance) |
Features | Corrosion Resistant |
| Fast Molding Cycle |
| Flame Retardant |
| Good Dimensional Stability |
| Good Processability |
| Heat Aging Resistant |
| High Flow |
| High Strength |
| Low Density |
Forms | Pellets |
Processing Method | Injection Molding |