A. Schulman BMC 605LWR Mineral Filled, Glass Fiber Reinforced Polyester Compound
Categories:
Polymer
;
Thermoset
;
Filled/Reinforced Thermoset
;
Polyester, TS
;
Thermoset Polyester Glass and Mineral Filled BMC
Material Notes:
BMC 605LWR is a mineral filled, glass fiber reinforced polyester bulk molding compound suitable for compression, transfer and stuffer injection molding. It is designed to provide improved wear resistance compared to standard BMC605.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.87
g/cc
1.87
g/cc
Water Absorption
0.10 %
0.10 %
24 hours, 23°C
Linear Mold Shrinkage
0.0020
-
0.0040
cm/cm
0.0020
-
0.0040
in/in
Mechanical Properties
Metric
English
Comments
Hardness, Barcol
15 - 20
15 - 20
Tensile Strength, Ultimate
27.6
-
48.3
MPa
4000
-
7000
psi
Flexural Strength
82.7
-
110
MPa
12000
-
16000
psi
Compressive Strength
117
-
138
MPa
17000
-
20000
psi
Izod Impact, Notched
1.60
-
2.67
J/cm
3.00
-
5.00
ft-lb/in
Electrical Properties
Metric
English
Comments
Dielectric Strength
11.8
-
13.0
kV/mm
300
-
330
kV/in
Short Time
Arc Resistance
>=
180
sec
>=
180
sec
Comparative Tracking Index
>=
600
V
>=
600
V
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
>=
260
°C
>=
500
°F
Flammability, UL94
V-0
@Thickness 6.35 mm
V-0
@Thickness 0.250 in
V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
Processing Properties
Metric
English
Comments
Mold Temperature
138
-
166
°C
280
-
330
°F
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
A. Schulman BMC 605 Mineral Filled, Glass Fiber Reinforced Polyester Compound
A. Schulman BMC 680 Mineral Filled, Glass Fiber Reinforced Polyester Compound
A. Schulman BMC 620X Mineral Filled, Glass Fiber Reinforced Polyester Compound
A. Schulman BMC 620M Mineral Filled, Glass Fiber Reinforced Polyester Compound
A. Schulman BMC 620 Mineral Filled, Glass Fiber Reinforced Polyester Compound
PBMC017 / 27200
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.