MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Adell ER-18 Homopolymer Polypropylene, 40% Glass Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Glass Fiber Filler

Material Notes: Data provided by Adell Plastics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³ASTM D792
Water Absorption 0.030 %0.030 %24 hour immersion; ASTM D570
Linear Mold Shrinkage 0.0035 cm/cm0.0035 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 6060ASTM D785
Hardness, Rockwell R 115115ASTM D785
Tensile Strength, Ultimate 96.5 MPa14000 psiASTM D638
Elongation at Break 2.5 %2.5 %ASTM D638
Flexural Strength 148 MPa21500 psiASTM D790
Flexural Modulus 6.80 GPa986 ksiASTM D790
Izod Impact, Notched 1.10 J/cm2.06 ft-lb/inASTM D256
Izod Impact, Unnotched 4.80 J/cm8.99 ft-lb/inASTM D256
Gardner Impact 0.300 J0.221 ft-lbASTM D3029
 
Thermal PropertiesMetricEnglishComments
Melting Point 182 °C360 °FASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 166 °C331 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 157 °C315 °FASTM D648
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Adell ER-38 Homopolymer Polypropylene, 40% Glass Reinforced
A. Schulman Lucent GPP-240 Homopolymer Polypropylene, 40% Glass Fiber Reinforced, Chemically Coupled
Polyram RamOfin PPH300G8 Polypropylene, 40% Glass Fiber
Plastcom SLOVALEN PH 69 GF 40 Polypropylene Homopolymer, 40% Glass Fiber
Omni Plastics OmniPro™ HPP GRC40 Homopolymer Polypropylene, 40% Glass reinforced

PDEL84 / 29647

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.