MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 Kendall® Extended Bearing Life (EBL) Grease NLGI Grade 0
Categories: Fluid; Lubricant; Urea Gellant

Material Notes: Kendall® Extended Bearing Life (EBL) Grease is a semifluid, extreme-pressure polyurea grease specially developed for the lubrication of wheel bearings on non-driven truck trailer axles equipped with oil seals. It is formulated to help optimize service intervals and reduce operating costs by providing effective lubrication and cooling of wheel bearings exposed to the prolonged high operating temperatures of over-the-road applications. EBL Grease is manufactured with high-quality base oils and a non-soap, polyurea thickener. It is fortified with extreme-pressure additives and rust and oxidation inhibitors to provide excellent wear protection, protection against rust and corrosion, and long service life. It has excellent thermal stability at high temperatures and excellent pumpability at low temperatures for use over a wide range of operating temperatures. It has excellent compatibility with elastomer seals and is resistant to water washout.

Applications:

  • Wheel bearings of non-driven trailer axles equipped with oil seals
Features/Benefits:
  • Excellent oxidation resistance and thermal stability at high temperatures
  • Excellent pumpability at low temperatures
  • Good load-carrying capacity
  • Protects against rust and corrosion
  • Resists water washout
  • Excellent seal compatibility
  • Formulated for extended service life

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.881 g/cc0.0318 lb/in³
Viscosity Measurement 9898Index
Saybolt Viscosity at 100°F 575 SUS575 SUS
Saybolt Viscosity at 210°F 68 SUS68 SUS
Kinematic Viscosity at 40°C (104°F) 110 cSt110 cSt
Kinematic Viscosity at 100°C (212°F) 12 cSt12 cSt
Oxidative Stability 100 hour
@Pressure 0.0345 MPa
100 hour
@Pressure 5.00 psi
Pressure Drop; ASTM D942
 
Mechanical PropertiesMetricEnglishComments
Four Ball Wear 0.400 mm0.0157 inScar Diameter; ASTM D2266
Penetration P(60), 1/10 mm 355 - 385355 - 385ASTM D217
Timken Test 18100 g40.0 lbASTM D2509
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -29.0 °C-20.2 °F
Dropping Point 204 °C399 °F
 
Descriptive Properties
ColorLight Green

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5325 / 198578

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.