MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ITW Spraycore® SC 4600 HTT Premium Vinyl Ester Tooling Resin
Categories: Polymer; Thermoset; Vinyl Ester

Material Notes: SC 4600 HTT is a promoted, vinyl ester blended premium mold building resin developed for the fabrication of FRP tooling in multiple pull and high temperature applications. Product features and benefits: excellent for high temperature applications. *Created with virtually zero shrink. *Improves laminate profile by elimination print through and surface distortion. *Helps increase balanced mold strength by up to 20%. * Offers significant labor cost reduction. *Minimizes pre-release. *Helps reduce cracking. *Reduces tooling costs by up to 25% when replacing balsa. Preferred red dye catalyst: MEKP 925, HP-90, DHD-9, L 50, K10.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 - 1.33 g/cc0.0450 - 0.0481 lb/in³Application density
Viscosity 7000 - 11000 cP7000 - 11000 cPRVF #5 @ 2.5/ 20rpm Thix index: 5.5-7.5
 
Chemical PropertiesMetricEnglishComments
Styrene Content 20 - 24 %20 - 24 %
 
Processing PropertiesMetricEnglishComments
Gel Time 12.0 - 20.0 min12.0 - 20.0 min
 20.0 - 30.0 min20.0 - 30.0 minGel to Peak
 
Descriptive Properties
ColorLight tan
Peak Exotherm210 to 255°F100g mass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWS9055 / 239565

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.