MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Mylar® M45 Polyester Film, 50 Gauge (15 µm), PVDC Coated  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyvinyl Dichloride (PVDC); Polyvinyl Dichloride (PVDC) Coated Polyester Film

Material Notes: Data provided by DuPont Packaging Polymers.

A transparent polyester packaging film, dispersion coated on one side with a PVDC copolymer. The coating is an excellent moisture and oxygen barrier. M45 is designed to be combined with a sealant layer, locking in the PVDC coating. M45 can be surface or reverse printed with appropriately formulated inks, and can be combined with other webs by adhesive or extrusion laminating. The coated surface is particularly well suited for water based inks and adhesives.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³Average value for Mylar® films.
Moisture Vapor Transmission 0.0900 cc-mm/m²-24hr-atm0.229 cc-mil/100 in²-24hr-atmASTM E96 Procedure E
Water Vapor Transmission 6.00 g/m²/day0.386 g/100 in²/dayASTM E96 Procedure E
Oxygen Transmission 0.0780 cc-mm/m²-24hr-atm0.198 cc-mil/100 in²-24hr-atmor 6 cc/m²-24hr-atm for the film. ASTM D3985
Thickness 15.0 microns0.591 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 155 %155 %ASTM D882
Film Elongation at Break, TD 120 %120 %ASTM D882
Modulus of Elasticity 3.45 GPa500 ksi(stiffness), ASTM D882
Tear Strength Test 300300Graves, g; ASTM D1004
Film Tensile Strength at Break, MD 152 MPa22000 psiASTM D882
Film Tensile Strength at Break, TD 179 MPa26000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °FNot cleared by FDA for food temperatures above this temperature.
Shrinkage 2.2 %
@Temperature 150 °C,
Time 1800 sec
2.2 %
@Temperature 302 °F,
Time 0.500 hour
Film shrinkage in oven.
 
Optical PropertiesMetricEnglishComments
Haze 7.0 %7.0 %ASTM D1003
Gloss 130 %130 %20°; ASTM D2457
Transmission, Visible 70 %70 %% Clarity; ASTM D1746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SK Chemicals Saran® 520 Vapor Retarder Tape
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/35%/UD134/AS7-12K
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/35%/150/AS7 GS
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy)
Hexcel® HexTow® IMA Intermediate Modulus Carbon Fiber (12,000 Filaments)

PDU681 / 33130

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.