MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

Sumitomo Bakelite FM 4004F Phenolic Novolac Compound
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Mineral/Glass Filled

Material Notes: FM 4004F is a fiberglass and mineral reinforced phenolic novolac compound with improved strength properties over FM 4004. This compound exhibits excellent dimensional stability and good strength at elevated temperatures.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.88 g/cc1.88 g/ccASTM D792
Apparent Bulk Density 0.975 g/cc0.0352 lb/in³Powder; ASTM D1895
Water Absorption  0.070 %
@Time 86400 sec
0.070 %
@Time 24.0 hour
ASTM D570
 0.15 %
@Time 173000 sec
0.15 %
@Time 48.0 hour
ASTM D570
Linear Mold Shrinkage 0.0023 cm/cm0.0023 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 123123ASTM D785
Tensile Strength 80.0 MPa11600 psiASTM D638
Flexural Strength 115 MPa16700 psiASTM D790
Flexural Modulus 17.1 GPa2480 ksiASTM D790
Compressive Strength 231 MPa33500 psiASTM D695
Izod Impact, Notched 0.290 J/cm0.543 ft-lb/inASTM D256A
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.6
@Frequency 1e+6 Hz
4.6
@Frequency 1e+6 Hz
wet; ASTM D150
Dielectric Strength  >= 14.4 kV/mm
@Frequency 60 Hz
>= 366 kV/in
@Frequency 60 Hz
SS
 >= 16.1 kV/mm
@Frequency 60 Hz
>= 409 kV/in
@Frequency 60 Hz
ST
Dissipation Factor 0.012
@Frequency 1e+6 Hz
0.012
@Frequency 1e+6 Hz
wet; ASTM D150
Arc Resistance 180 sec180 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 19.0 µm/m-°C10.6 µin/in-°FASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 185 °C365 °FAs Molded; ASTM D648A
 >= 282 °C>= 540 °FPost Baked; ASTM D648A
Flammability, UL94  V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
 
Descriptive Properties
UL Temperature Index150UL 746B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite Sumikon® PM-3025 Phenolic Novolac
Sumitomo Bakelite FM 4004 Phenolic Novolac Compound
Sumitomo Bakelite Sumikon® PM-3028 Phenolic Novolac
Sumitomo Bakelite Sumikon® PM-9630 Type JK Black Phenolic Resol
Sumitomo Bakelite Sumikon® PM-9630 Type J Black Phenolic Resol

PSUMIT156 / 193961

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.