MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chi Mei Polylac® PA-765B ABS - Flame Retardant
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes: F.R. Medium Impact

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/inASTM D955
Melt Flow  4.2 g/10 min
@Load 5.00 kg,
Temperature 200 °C
4.2 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 42 g/10 min
@Load 10.0 kg,
Temperature 220 °C
42 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ISO-1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 102102ASTM D785
Ball Indentation Hardness 82.0 MPa11900 psiH358/30; ISO 2039-1
Tensile Strength at Break 30.0 MPa4350 psi50 mm/min; ISO 527
Tensile Strength, Yield 41.0 MPa5950 psi50 mm/min; ISO 527
Elongation at Break 10 %10 %50 mm/min; ISO 527
Flexural Strength 57.0 MPa8270 psi2 mm/min; ISO 178
Flexural Modulus 1.80 GPa261 ksi2 mm/min; ISO 178
Izod Impact, Notched  2.22 J/cm
@Thickness 6.35 mm
4.16 ft-lb/in
@Thickness 0.250 in
ASTM D256
 2.66 J/cm
@Thickness 3.17 mm
4.98 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Notched (ISO) 20.0 kJ/m²9.52 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) NBNBISO 180/1C
Charpy Impact Unnotched NBNBISO 179
Charpy Impact, Notched 2.00 J/cm²9.52 ft-lb/in²ISO 179
Impact 1313Impact Flexural Test Notched (KJ/m²)
 NBNBImpact Flexural Test Unnotched (KJ/m²)
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C171 °Funannealed; ISO 75
 91.0 °C196 °Fannealed; ISO 75
Vicat Softening Point  79.0 °C
@Load 5.00 kg
174 °F
@Load 11.0 lb
50°C/hr; ISO 306
 82.0 °C
@Load 5.00 kg
180 °F
@Load 11.0 lb
120°C/hr; ISO 306
 90.0 °C
@Load 1.00 kg
194 °F
@Load 2.20 lb
50°C/hr; ISO 306
 92.0 °C
@Load 1.00 kg
198 °F
@Load 2.20 lb
120°C/hr; ISO 306
Flammability, UL94  V-2
@Thickness 2.12 mm
V-2
@Thickness 0.0833 in
UL 94
 V-0
@Thickness 2.54 mm
V-0
@Thickness 0.100 in
UL 94
 5VA
@Thickness 3.17 mm
5VA
@Thickness 0.125 in
UL 94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chi Mei Polylac® PA-765A ABS - Flame Retardant
Chi Mei Polylac® PA-765 ABS - Flame Retardant
Overview of materials for Polypropylene, Flame Retardant
Chi Mei Polylac® PA-764 ABS - Flame Retardant
Chi Mei Polylac® PA-763 ABS - Flame Retardant

PCHI922 / 109410

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.