MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Goodfellow Polyaramid/Vinylester Composite Tube or Rod
Categories: Polymer; Thermoset; Vinyl Ester

Material Notes: Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 - 1.40 g/cc0.0434 - 0.0506 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 800 - 1000 MPa116000 - 145000 psiLongitudinal
Elongation at Break 2.5 %2.5 %Longitudinal
Flexural Strength 150 - 250 MPa21800 - 36300 psiLongitudinal
Flexural Modulus 17.0 - 22.0 GPa2470 - 3190 ksiLongitudinal
Compressive Strength 100 - 300 MPa14500 - 43500 psiLongitudinal
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Descriptive Properties
Volume Fraction Fibers, %50-60

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Applied Composites 8079 Modified Vinylester SMC
Applied Composites 175 Vinylester SMC
Polynt POLYCOR® VINYLESTER TOOLING GELCOAT PA
Sumitomo Bakelite RX® 1310 Diallyl Ortho-Phthalate Molding Compound
Bedford Plastics Glass Reinforced Vinylester Structural Fiberglass Profiles

PGOODF214 / 42285

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.