MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions Vinyl Rigid Extrusion 85883  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade; PVC, Sheet Grade

Material Notes: The Cell Classification was determined using the notched Izod test with injection molded samples.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.38 g/cc1.38 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 83
@Time 15.0 sec
83
@Time 0.00417 hour
ASTM D2240
Tensile Strength, Yield 50.4 MPa7310 psiType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.71 GPa393 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 84.3 MPa12200 psiASTM D790
Flexural Modulus 2.78 GPa403 ksiASTM D790
Izod Impact, Notched  1.28 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
2.40 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Across Flow, Compression Molded; ASTM D256A
 1.55 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
2.90 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Flow, Compression Molded; ASTM D256A
Dart Drop Total Energy  62.3 J/cm
@Temperature 23.0 °C
0.117 ft-lb/mil
@Temperature 73.4 °F
Procedure A, C.125 Dart; ASTM D4226
 153 J/cm
@Temperature 23.0 °C
0.287 ft-lb/mil
@Temperature 73.4 °F
Procedure B, C.125 Dart; ASTM D4226
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 74.0 µm/m-°C41.1 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
@Thickness 3.18 mm
160 °F
@Thickness 0.125 in
Unannealed; ASTM D648
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
All colors; UL 94
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
All colors; UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 193 °C360 - 379 °F
 
Descriptive Properties
FeaturesHigh Gloss
FormsPellets
Processing MethodSheet Extrusion
 Thermoforming
PVC Cell Classification13454ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesOutdoor Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for PVC, Sheet Grade
Karina BR-11 White PVC Compound
Geon® Performance Solutions 87725 Sheet PVC
Geon® Performance Solutions 87655 Sheet PVC
Chi Mei Wonderloy® PC-510 PC/ABS Alloy - Flame Retardant

PH1PN8738 / 102574

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.