MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger Tecapeek® CMP natural Polyetheretherketone
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes:
  • good heat deflection temperature
  • good machinability
  • inherent flame retardant
  • hydrolysis and superheated steam
  • resistant
  • resistance against high energy radiation
  • good slide and wear properties
  • high toughness
  • high creep resistance
Target Industries:
  • semiconductor technology

Information provided by Ensinger Inc.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³
Water Absorption  0.020 %
@Time 86400 sec
0.020 %
@Time 24.0 hour
DIN EN ISO 62
 0.030 %
@Time 346000 sec
0.030 %
@Time 96.0 hour
DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 240 MPa34800 psiISO 2039-1
Tensile Strength 110 MPa16000 psi50mm/min; DIN EN ISO 527-2
Elongation at Break 50 %50 %50 mm/min; DIN EN ISO 527-1
Elongation at Yield 4.0 %4.0 %50 mm/min; DIN EN ISO 527-1
Modulus of Elasticity 4.10 GPa595 ksi1mm/min; DIN EN ISO 527-2
Flexural Strength 160 MPa
@Load 1.02 kg
23200 psi
@Load 2.25 lb
2mm/min; DIN EN ISO 178
Flexural Modulus 3.90 GPa
@Load 1.02 kg
566 ksi
@Load 2.25 lb
2mm/min; DIN EN ISO 178
Compressive Strength  15.0 MPa
@Strain 1 %,
Load 1.02 kg
2180 psi
@Strain 1 %,
Load 2.25 lb
5mm/min; EN ISO 604
 34.0 MPa
@Strain 2 %,
Load 1.02 kg
4930 psi
@Strain 2 %,
Load 2.25 lb
5mm/min; EN ISO 604
Compressive Modulus 3.20 GPa
@Load 1.02 kg
464 ksi
@Load 2.25 lb
5mm/min; EN ISO 604
Charpy Impact Unnotched NBNBmax. 7,5J; DIN EN ISO 179-1eU
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²DIN EN ISO 179-1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmSilver electrode, 23°C, 12% r.h.; DIN IEC 60093
Surface Resistivity per Square 1.00e+15 ohm1.00e+15 ohmSilver electrode, 23°C, 12% r.h.; DIN IEC 60093
Dielectric Strength 73.0 kV/mm1850 kV/inISO 60243-1
Comparative Tracking Index 125 V125 VPlatin electrode, 23°C, 50% r.h., solvent A; DIN EN 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  50.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
27.8 µin/in-°F
@Temperature 73.4 - 140 °F
DIN EN ISO 11359-1;2
 60.0 µm/m-°C
@Temperature 23.0 - 100 °C
33.3 µin/in-°F
@Temperature 73.4 - 212 °F
DIN EN ISO 11359-1;2
 70.0 µm/m-°C
@Temperature 100 - 150 °C
38.9 µin/in-°F
@Temperature 212 - 302 °F
DIN EN ISO 11359-1;2
Specific Heat Capacity 1.10 J/g-°C0.263 BTU/lb-°FISO 22007-4:2008
Thermal Conductivity 0.270 W/m-K1.87 BTU-in/hr-ft²-°FISO 22007-4:2008
Melting Point 340 °C644 °FDIN EN ISO 11357
Maximum Service Temperature, Air 260 °C500 °Flong term
 300 °C572 °Fshort term
Deflection Temperature at 1.8 MPa (264 psi) 162 °C324 °FISO-R 75 Method A
Glass Transition Temp, Tg 151 °C304 °FDIN EN ISO 11357
 
Descriptive Properties
Colorbeige opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8180 / 319108

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.