MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Oxygen-free Electronic Copper (OFE), UNS C10100, O61 Temper Bar
Categories: Metal; Nonferrous Metal; Copper Alloy; Wrought Copper

Material Notes: Applications: busbars, bus conductors, waveguides, hollow conductors, lead-in wires and anodes for vacuum tubes, vacuum seals, transistor components, glass-to-metal seals, coaxial cables, klystrons, microwave tubes, and rectifiers.

Processing: Excellent hot and cold workability; good forgeability. Fabricated by bending, coining, coppersmithing, drawing and upsetting, hot forging and pressing, knurling, roll threading, shearing, spinning, swaging, and stamping.

Corrosion Resistance: Good to excellent. Susceptible to galvanic corrosion when coupled with iron, aluminum, magnesium, lead, tin, and zinc. Good resistance to atmospheric, brackish water, sea water, and non-oxidizing acid corrosion, but avoid heating in oxidizing atmospheres or exposing to oxidizing acids, moist halogens, sulfides, ammonia, or solutions with ammonium ions.

UNS C10100 - ASTM B48, B133, B152, B187, B272, B432, F68; 101A (Australia); C110 (UK); CDA 101 OFE; ISO Cu-OFE; JIS C1011 H3510 (Japan)

Key Words: ISO Cu-OFE, CEN CW009A, oxygen-free high conductivity copper (OFHC), CDA 101 OFE, ASTM B48, B133, B152, B187, B272, B432, F68, AS 101A 1567 (Australia), Cu/cl NF A53301, JIS C1011 H3510, flat products, plates, sheets, strips
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  240 MPa
@Temperature 0.000 °C
34800 psi
@Temperature 32.0 °F
 250 MPa
@Temperature -50.0 °C
36300 psi
@Temperature -58.0 °F
 285 MPa
@Temperature -100 °C
41300 psi
@Temperature -148 °F
 325 MPa
@Temperature -150 °C
47100 psi
@Temperature -238 °F
 365 MPa
@Temperature -200 °C
52900 psi
@Temperature -328 °F
 410 MPa
@Temperature -250 °C
59500 psi
@Temperature -418 °F
Tensile Strength, Yield  70.0 MPa
@Strain 0.2 %,
Temperature -50.0 °C
10200 psi
@Strain 0.2 %,
Temperature -58.0 °F
 70.0 MPa
@Strain 0.2 %,
Temperature 0.000 °C
10200 psi
@Strain 0.2 %,
Temperature 32.0 °F
 72.0 MPa
@Strain 0.2 %,
Temperature -100 °C
10400 psi
@Strain 0.2 %,
Temperature -148 °F
 78.0 MPa
@Strain 0.2 %,
Temperature -150 °C
11300 psi
@Strain 0.2 %,
Temperature -238 °F
 85.0 MPa
@Strain 0.2 %,
Temperature -200 °C
12300 psi
@Strain 0.2 %,
Temperature -328 °F
 94.0 MPa
@Strain 0.2 %,
Temperature -250 °C
13600 psi
@Strain 0.2 %,
Temperature -418 °F
Elongation at Break  51 %
@Temperature -100 °C
51 %
@Temperature -148 °F
 51 %
@Temperature -50.0 °C
51 %
@Temperature -58.0 °F
 52 %
@Temperature 0.000 °C
52 %
@Temperature 32.0 °F
 55 %
@Temperature -150 °C
55 %
@Temperature -238 °F
 60 %
@Temperature -200 °C
60 %
@Temperature -328 °F
 69 %
@Temperature -250 °C
69 %
@Temperature -418 °F
Modulus of Elasticity 115 GPa16700 ksi
Poissons Ratio 0.310.31
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Forgeability 65 %65 %UNS C37700 (forging brass) = 100%
Shear Modulus 44.0 GPa6380 ksi
Charpy Impact  72.0 J
@Temperature 0.000 °C
53.1 ft-lb
@Temperature 32.0 °F
V Notch
 74.0 J
@Temperature -50.0 °C
54.6 ft-lb
@Temperature -58.0 °F
V Notch
 79.0 J
@Temperature -100 °C
58.3 ft-lb
@Temperature -148 °F
V Notch
 89.0 J
@Temperature -150 °C
65.6 ft-lb
@Temperature -238 °F
V Notch
 90.0 J
@Temperature -250 °C
66.4 ft-lb
@Temperature -418 °F
V Notch
 92.0 J
@Temperature -200 °C
67.9 ft-lb
@Temperature -328 °F
V Notch
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000171 ohm-cm
@Temperature 20.0 °C
0.00000171 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  17.0 µm/m-°C
@Temperature 20.0 - 100 °C
9.44 µin/in-°F
@Temperature 68.0 - 212 °F
 17.3 µm/m-°C
@Temperature 20.0 - 200 °C
9.61 µin/in-°F
@Temperature 68.0 - 392 °F
 17.7 µm/m-°C
@Temperature 20.0 - 300 °C
9.83 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.385 J/g-°C
@Temperature 20.0 °C
0.0920 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 391 W/m-K
@Temperature 20.0 °C
2710 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1083 °C1981 °F
Annealing Point >= 371 °C>= 700 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 375 - 650 °C707 - 1200 °F
Hot-Working Temperature 750 - 875 °C1380 - 1610 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu >= 99.99 %>= 99.99 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Oxygen-free electronic Copper, UNS C10100
Oxygen-free Electronic Copper (OFE), UNS C10100, H80 (16%) Temper, rod
Oxygen-free Electronic Copper (OFE), UNS C10100, H80 (35%), rod (25 mm Diameter)
Oxygen-free Electronic Copper (OFE), UNS C10100, OS050 temper, wire
Oxygen-free Electronic Copper (OFE), UNS C10100, H04 Temper, flat products

MC10100d4 / 171671

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.