MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EPICHEM Epilon PC IX3000 Polycarbonate, High Impact  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Impact Modified

Material Notes: Characteristics: high fluidity, high impact

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792, ISO 1183
Water Absorption 0.15 %
@Temperature 23.0 °C
0.15 %
@Temperature 73.4 °F
24h; ASTM D570, ISO 62
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Index of Compound 15 - 20 g/10 min
@Load 1.20 kg,
Temperature 300 °C
15 - 20 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238, ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 7070ASTM D785, ISO 2039/2
Tensile Strength, Yield 58.0 MPa8410 psiASTM D638, ISO R527
Elongation at Break >= 100 %>= 100 %ASTM D638, ISO R527
Flexural Strength 93.0 MPa13500 psiASTM D790, ISO 178
Flexural Modulus 2.43 GPa352 ksiASTM D790, ISO 178
Izod Impact, Notched  0.900 - 1.70 J/cm
@Thickness 3.20 mm,
Temperature -40.0 °C
1.69 - 3.18 ft-lb/in
@Thickness 0.126 in,
Temperature -40.0 °F
ASTM D256, ISO 180/4a
 >= 5.00 J/cm
@Thickness 3.20 mm,
Temperature 0.000 °C
>= 9.37 ft-lb/in
@Thickness 0.126 in,
Temperature 32.0 °F
ASTM D256, ISO 180/4a
 6.00 - 8.00 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
11.2 - 15.0 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256, ISO 180/4a
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+14 ohm1.00e+14 ohmASTM D257, IEC 93
Dielectric Constant 3.0
@Frequency 1000 Hz
3.0
@Frequency 1000 Hz
ASTM D150, IEC 250
Dielectric Strength 35.0 kV/mm889 kV/inASTM D149, IEC 243
Dissipation Factor 0.0010
@Frequency 1000 Hz
0.0010
@Frequency 1000 Hz
ASTM D150, IEC 250
Comparative Tracking Index 180 V180 VVDE 0303-P1, IEC 112
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 110 °C230 °F20000 h; VDE 0304/P2-1, IEC 216
 115 °C239 °F5000 h; VDE 0304/P2-1, IEC 216
 135 °C275 °Ffew hours; VDE 0304/P2-1, IEC 216
Hot Ball Pressure Test >= 128 °C>= 262 °FBS 3456, IEC 335
Deflection Temperature at 1.8 MPa (264 psi) 138 °C280 °FASTM D648, ISO 75
Vicat Softening Point  138 - 145 °C
@Load 5.00 kg
280 - 293 °F
@Load 11.0 lb
120°C/hr; ASTM D1525/B, ISO 306/B
 150 - 155 °C
@Load 0.999 kg
302 - 311 °F
@Load 2.20 lb
120°C/hr; ASTM D1525/A, ISO 306/A
Flammability, UL94  V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
 V-2
@Thickness 3.20 mm
V-2
@Thickness 0.126 in
Glow Wire Test  750 °C
@Thickness 3.20 mm
1380 °F
@Thickness 0.126 in
VDE 0471/P2-4, IEC 695
 750 °C
@Thickness 2.00 mm
1380 °F
@Thickness 0.0787 in
VDE 0471/P2-4, IEC 695
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.541.54ASTM D542, ISO R489
Transmission, Visible 88 - 90 %88 - 90 %ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEPI019 / 82841

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.