MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Impet® 740 PET, 45% Glass/Mineral Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced

Material Notes:

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.72 g/cc0.0621 lb/in³ISO 1183
Water Absorption 0.060 %0.060 %ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 140 MPa20300 psiISO 527
Elongation at Break 1.4 %1.4 %ASTM D638
Flexural Strength 215 MPa31200 psiISO 178
Flexural Modulus 15.6 GPa2260 ksiISO 178
Izod Impact, Notched 0.700 J/cm1.31 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.9
@Frequency 100000 Hz
3.9
@Frequency 100000 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
@Thickness 3.17 mm
432 kV/in
@Thickness 0.125 in
ASTM D149
Dissipation Factor 0.010
@Frequency 100000 Hz
0.010
@Frequency 100000 Hz
ASTM D150
Arc Resistance 126 sec126 secASTM D495
Comparative Tracking Index 200 V200 VASTM D3638
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.6 µm/m-°C
@Temperature 20.0 °C
17.0 µin/in-°F
@Temperature 68.0 °F
ASTM E831
CTE, linear, Transverse to Flow 103 µm/m-°C
@Temperature 20.0 °C
57.2 µin/in-°F
@Temperature 68.0 °F
ASTM E831
Melting Point 248 °C478 °FDSC; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 245 °C473 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 228 °C442 °FASTM D648
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature 270 - 280 °C518 - 536 °FInjection; barrel center zone temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHCU75 / 45815

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.