MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

North Wood Plastics 60 HDPE + UNIFILL (20% Wood Fiber)  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Wood Filled

Material Notes: Data provided by North Wood Plastics, Inc. UNIFILL-60 is a general purpose polyolefin compound compatible in both PP and HDPE. It is a masterbatch with 60% high quality pine wood flour filler. It is made with only the highest quality recycled resins. 2:1 HDPE:UNIFILL-60 yields an end product with 20% fiber.

Key Words: Wood Flour; High Density Polyethylene; Recycled Polyolefin
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.994 g/cc0.0359 lb/in³ASTM D792
Linear Mold Shrinkage 0.012 cm/cm0.012 in/inASTM D955
Melt Flow 2.0 g/10 min
@Temperature 190 °C
2.0 g/10 min
@Temperature 374 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 15.0 MPa2180 psiASTM D638
Elongation at Break 15 %15 %ASTM D638
Tensile Modulus 1.80 GPa261 ksiASTM D638
Flexural Yield Strength 38.0 MPa5510 psiASTM D790
Flexural Modulus 1.20 GPa174 ksiASTM D790
Izod Impact, Notched 0.430 J/cm0.806 ft-lb/inASTM D256
Izod Impact, Unnotched 2.40 J/cm4.50 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 43.0 °C109 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 200 °C<= 392 °FTo prevent fiber degradation.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
North Wood Plastics 60 PP + UNIFILL (20% Wood Fiber)
Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane
LG Chemical SEETEC PB270 HDPE
FKuR Kunststoff Terralene® HD 3505 Biobased Polyethylene
FKuR Kunststoff Fibronlon® S 7530 Wood-Plastic Composite

PWOOD92 / 20257

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.