MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Quantum Composites QC-7752 50% Glass Fiber Heat Resistant Polyester SMC  (discontinued **)
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: QC-7752 is a modified polyester sheet molding compound (SMC) that is designed for applications requiring high strength, good environmental resistance, and resistance to elevated temperatures. It offers fast molding cycles and good surface appearance. Form and Colors = Roll, Off White/Black/Gray. Glass Length = 1 inch.

A. Schulman has acquired Quantum Composites.

Key Words: Sheet Molding Compound
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.85 g/cc0.0668 lb/in³ASTM D792
Water Absorption 0.15 %0.15 %ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 5858ASTM D2583
Tensile Strength, Ultimate 193 MPa28000 psiASTM D638
Tensile Modulus 17.9 GPa2600 ksiASTM D638
Flexural Yield Strength 310 MPa45000 psiASTM D790
Flexural Modulus 14.5 GPa2100 ksiASTM D790
Compressive Yield Strength 172 MPa24900 psiASTM D695
Izod Impact, Notched 14.4 J/cm27.0 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Shrinkage 0.0010 %0.0010 %
 
Processing PropertiesMetricEnglishComments
Processing Temperature 132 - 157 °C270 - 315 °FMold temperature

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Haysite 46000 Polyester SMC, 30% Glass Reinforced
IDI Composites Rosite® C200BS ESD SMC, Conductive Thermoset Polyester, 10% Glass Reinforced
Menzolit Menzolit® SMC 0180 Unsaturated Polyester UP
Menzolit Menzolit® SMC 0600 Unsaturated Polyester UP
Menzolit Menzolit® SMC 2600 Unsaturated Polyester UP

PCOQC4 / 29041

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.