MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Toyobo Zenite® SEA 10 N LCP, 30% Mineral Fiber Reinforced
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Mineral Filled

Material Notes: Product Description: Zenite SEA 10 N is a 30% mineral filled grade. It offers excellent antistatic property, surface appearance, low warpage, and excellent dimensional stability. Application for this grade is compact camera module, and other thin, small electronic parts.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Filler/Reinforcement: Mineral

Additive: Antistatic

Features: Antistatic; Low Warpage

Form: Pellets

Processing Method: Injection Molding

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.64 g/cc0.0592 lb/in³ISO 1183
Water Absorption 0.020 %0.020 %Equilibrium, 50% RH; ISO 62
Maximum Moisture Content 0.0100.010
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 130 MPa18900 psiISO 527-2/5
Elongation at Break 2.3 %2.3 %ISO 527-2/5
Tensile Modulus 13.0 GPa1890 ksiISO 527-1
Flexural Strength 150 MPa21800 psiISO 178
Flexural Modulus 13.0 GPa1890 ksiISO 178
Flexural Strain at Break 2.3 %2.3 %ISO 178
Charpy Impact, Notched 1.01 J/cm²4.80 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.30e+12 ohm-cm2.30e+12 ohm-cmIEC 62631-3-1
Surface Resistance 9.80e+11 ohm9.80e+11 ohmIEC 62631-3-2
Dielectric Strength 38.2 kV/mm970 kV/inAC; IEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.1 µm/m-°C5.60 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 59.4 µm/m-°C33.0 µin/in-°FISO 11359-2
Specific Heat Capacity 0.00138 J/g-°C0.000330 BTU/lb-°FISO 22007-4
Thermal Conductivity 0.476 W/m-K3.30 BTU-in/hr-ft²-°FThruplane; ISO 22007-4
 0.893 W/m-K6.20 BTU-in/hr-ft²-°FCrossflow; ISO 22007-4
 2.45 W/m-K17.0 BTU-in/hr-ft²-°FFlow; ISO 22007-4
Melting Point 330 °C626 °FISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 240 °C464 °FUnannealed; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 310 - 320 °C590 - 608 °F
Middle Barrel Temperature 320 - 330 °C608 - 626 °F
Front Barrel Temperature 330 - 350 °C626 - 662 °F
Nozzle Temperature 330 - 340 °C626 - 644 °F
Zone 4 330 - 350 °C626 - 662 °FInjection
Melt Temperature 335 - 345 °C635 - 653 °F
Mold Temperature 80.0 - 140 °C176 - 284 °F
Drying Temperature 150 °C302 °F
Dry Time 6.00 hour6.00 hour
Injection Pressure 50.0 - 150 MPa7250 - 21800 psi
 
Descriptive Properties
Thermal DiffusivityCrossflow, ISO 22007-4
 Flow, ISO 22007-4
 Thruplane, ISO 22007-4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHCQ6332 / 311025

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.