MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Corning XDF DARK GRAY Tinted Photochromic Glass
Categories: Ceramic; Glass; Optical

Material Notes: Application : Pretinted 45% photochromic glass suited for general or special purpose Tinted Glasses. Neutral gray with excellent color rendition. Pass cited standards for traffic signal recognition at 2 mm thickness. Blanks for corrective lenses available on request.

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.41 g/cc0.0871 lb/in³
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.50 µm/m-°C
@Temperature 20.0 - 300 °C
3.61 µin/in-°F
@Temperature 68.0 - 572 °F
Softening Point 665 °C1230 °F
Annealing Point 495 °C923 °F
Strain Point 665 °C1230 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.52017
@Wavelength 656.3 nm
1.52017
@Wavelength 656.3 nm
Line: C; Hydrogen
 1.52064
@Wavelength 643.8 nm
1.52064
@Wavelength 643.8 nm
Line: C'; Cadmium
 1.523
@Wavelength 587.6 nm
1.523
@Wavelength 587.6 nm
Line: d; Helium
 1.52518
@Wavelength 546.1 nm
1.52518
@Wavelength 546.1 nm
Line: e; Mercury
 1.52933
@Wavelength 486.1 nm
1.52933
@Wavelength 486.1 nm
Line: F; Hydrogen
 1.52992
@Wavelength 480 nm
1.52992
@Wavelength 480 nm
Line: F'; Cadmium
Abbe Number 56.656.6ve
 5757vd
Transmission, Visible  15.5 %
@Wavelength 380 - 780 nm,
Thickness 2.00 mm
15.5 %
@Wavelength 380 - 780 nm,
Thickness 0.0787 in
Luminous, Darkened
 16 %
@Wavelength 380 - 500 nm,
Thickness 2.00 mm
16 %
@Wavelength 380 - 500 nm,
Thickness 0.0787 in
Blue light transmission factor, Darkened
 44 %
@Wavelength 380 - 780 nm,
Thickness 2.00 mm
44 %
@Wavelength 380 - 780 nm,
Thickness 0.0787 in
Luminous, Faded
 45 %
@Wavelength 380 - 500 nm,
Thickness 2.00 mm
45 %
@Wavelength 380 - 500 nm,
Thickness 0.0787 in
Blue light transmission factor, Faded
UV Transmittance  <= 0.10 %
@Thickness 2.00 mm
<= 0.10 %
@Thickness 0.0787 in
Solar UV-B transmission factor, Faded
 <= 0.10 %
@Thickness 2.00 mm
<= 0.10 %
@Thickness 0.0787 in
Solar UV-B transmission factor, Darkened
 1.5 %
@Thickness 2.00 mm
1.5 %
@Thickness 0.0787 in
Solar UV-A transmission factor, Darkened
 4.5 %
@Thickness 2.00 mm
4.5 %
@Thickness 0.0787 in
Solar UV-A transmission factor, Faded
 <= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 2.00 mm
<= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 0.0787 in
t(max), Faded
 <= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 2.00 mm
<= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 0.0787 in
t(max), Darkened
 <= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 2.00 mm
<= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 0.0787 in
t(avg), Faded
 <= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 2.00 mm
<= 0.10 %
@Wavelength 280 - 315 nm,
Thickness 0.0787 in
t(avg), Darkened
 1.0 %
@Wavelength 315 - 350 nm,
Thickness 2.00 mm
1.0 %
@Wavelength 315 - 350 nm,
Thickness 0.0787 in
t(max), Darkened
 2.0 %
@Wavelength 380 - 500 nm,
Thickness 2.00 mm
2.0 %
@Wavelength 380 - 500 nm,
Thickness 0.0787 in
t(moy), Darkened
 3.0 %
@Wavelength 315 - 350 nm,
Thickness 2.00 mm
3.0 %
@Wavelength 315 - 350 nm,
Thickness 0.0787 in
t(max), Faded
 7.0 %
@Wavelength 380 - 500 nm,
Thickness 2.00 mm
7.0 %
@Wavelength 380 - 500 nm,
Thickness 0.0787 in
t(moy), Faded
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
96% Silica Consolidated Reconstructed Glass
Corning XDF LIGHT GRAY Tinted Photochromic Glass
Corning Unicrown Chemtemperable, UV absorbing crown glass
Corning FUMO 15 Tinted Optical Glass
Borosilicate Glass, Low Expansion

CCORN928 / 233339

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.