Exxtra™ Soft EMA2022 is an ethylene methyl acrylate copolymer. Exxtra™ Soft EMA2022 can be used for injection molding applications. It can be used in alloys, blends or compounds to increase impact strength or to lower the modulus. Exxtra™ Soft EMA2022 can be injection molded and extruded Availability: Latin America, North America. Additive: antiblock: no; slip: no; thermal stabilizer: yes Applications: Compatibilizer; Engineering thermoplastic impact modifier; Foams; Injection Molding; Soft, molded parts Information provided by ExxonMobil. |