MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Mocom (ALBIS) ALCOM® PC+ABS 750/10 GF10 RD1016-05LB PC+ABS, 10% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Glass Fiber Filled

Material Notes: Base Polymer: Polycarbonate + Acrylonitrile Butadiene Styrene Blend

Filler/Additive System: 10% glass fibers, special filler

Color: Red, similar to RAL 3013

Special Features: Opaque

Market Segment: Automotive, Lighting

Application Area: Light transparent components

Typical Application: Display elements, operating elements

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³ISO 1183
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cm
@Time 86400 sec
0.0020 - 0.0060 in/in
@Time 24.0 hour
ISO 294-4
Melt Flow 16 g/10 min
@Load 5.00 kg,
Temperature 260 °C
16 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ISO 1133
Storage Temperature <= 30.0 °C<= 86.0 °Fdry, protected from light
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 60.0 MPa8700 psiISO 527
Elongation at Break 5.0 %5.0 %ISO 527
Tensile Modulus 3.45 GPa500 ksiISO 527
Flexural Strength 100 MPa14500 psiISO 178
Flexural Modulus 3.45 GPa500 ksiISO 178
Charpy Impact Unnotched 3.50 J/cm²16.7 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 128 °C262 °FB50; ISO 306
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 0.20 %
@Thickness 0.500 mm
0.20 %
@Thickness 0.0197 in
Y10; ISO 13468
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 280 °C428 - 536 °FInjection molding
Mold Temperature 70.0 - 100 °C158 - 212 °FInjection molding
Drying Temperature  100 - 110 °C
@Time 7200 - 14400 sec
212 - 230 °F
@Time 2.00 - 4.00 hour
in a dry air (desiccant) dryer
 100 - 110 °C
@Time 14400 - 28800 sec
212 - 230 °F
@Time 4.00 - 8.00 hour
in an circulating dryer
 
Descriptive Properties
Base PolymerPolycarbonate + Acrylonitrile Butadiene Styrene Blend

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Versalis KOBLEND PCA PD 935 G2 PC+ABS, 10% Glass Fiber
Avient Edgetek® CY-20GF/000 UV FR V0 PC/ABS Blend, Glass Filled
Polykemi AB POLYblend 45FS GF20 PC/ABS-Blend, Glass Fiber reinforced
Techmer ES HiFill® ABS GF5 5% Glass Filled
Polymer Resources PC/ABS-G10 General Purpose PC/ABS Alloy, 10% Glass Filled

PALBIS8565 / 242624

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.