MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

North American Sycamore Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Diffuse-Porous Hardwood. Data is based on small, clear, air-dried samples unless specified.

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Platanus occidentalis; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.460 g/cc0.0166 lb/in³Oven Dry Weight/Unseasoned Volume
 0.833 g/cc0.0301 lb/in³Unseasoned*
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 2700 N607 lb (f)Side. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 3100 N697 lb (f)End. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 3400 N764 lb (f)Side
Tensile Strength, Ultimate 4.34 MPa630 psiPerpendicular to Grain*
 5.00 MPa725 psiPerpendicular to Grain
Modulus of Rupture 0.0448 GPa6.50 ksiStatic Bending*
 0.0690 GPa10.0 ksiStatic Bending
Flexural Yield Strength 22.8 MPa3300 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 7.31 GPa1060 ksiStatic Bending*
 9.80 GPa1420 ksiStatic Bending
Compressive Strength 3.10 MPa450 psiPerpendicular to Grain*
 4.80 MPa696 psiPerpendicular to Grain
 16.5 MPa2390 psiParallel to Grain*
 20.1 MPa2920 psiMax Crushing Strength Parallel to Grain*
 37.0 MPa5370 psiParallel to Grain
Shear Strength 6.89 MPa1000 psiParallel to Grain*
 10.1 MPa1460 psiOrientation Unknown
Impact 3.33.3in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 88008800psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.00414 J/cm³0.600 in-lb/in³Static Bending*
Work to Maximum Load 0.0517 J/cm³7.50 in-lb/in³Static Bending*
Cleavage 46.0 kN/m262 lb/inRadial surface of failure, Unseasoned*
 74.0 kN/m422 lb/inTangential surface of failure, Unseasoned*
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.124 W/m-K0.860 BTU-in/hr-ft²-°FOven Dry
 0.144 W/m-K1.00 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 5.1 %5.1 %Radial; Green to Zero Moisture
 7.6 %7.6 %Tangential; Green to Zero Moisture
 14.2 %14.2 %Volumetric; Green to Zero Moisture

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Hickory Wood
American Red Maple Wood
North American Cherry (Black Cherry) Wood
North American Loblolly Pine Wood
North American Northern Red Oak Wood

PTSA180 / 71256

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.